Titanium alloys are widely used in various engineering design application due to its superior material properties. The traditional manufacturing of titanium products is always difficult, time consuming, high material wastage and manufacturing costs. Selective laser melting (SLM), an additive manufacturing technology has widely gained attention due to its capability to produce near net shape components with less production time. In this technical paper,microstructure,chemical composition,tensile properties and hardness are studied for the wrought and additive manufactured SLM cylindrical bar. Microstructure,mechanical properties and hardness were studied in both the longitudinal and transverse directions of the bar to study the effect of orientation. It was found that additive manufactured bar have higher yield strength, ultimate tensile strength and hardness than the wrought bar. For both conventional and SLM test samples, the yield strength, ultimate tensile strength and hardness was found to be high in the transverse direction. The difference in the properties can be attributed to the difference in microstructure as a result of processing conditions. The tensile fracture area was quantified by careful examination of the fracture surfaces in the scanning electron microscope
In this paper, the effect of machining parameters such as cutting speed and feed rate on cutting forces and surface roughness during turning of wrought and additive manufactured titanium alloys Ti-6Al-4V (selective laser melting) was studied. It was found that high cutting speeds and feed rates resulted in high cutting forces and poor surface finish. It was also found that higher cutting forces were required for machining selective laser melted titanium alloy (SLM Ti-6Al-4V) as compared to that of conventionally produced wrought Ti-6Al-4V due to the higher strength and hardness of SLM Ti-6Al-4V. After machining, surface roughness of additive manufactured titanium alloys was found to be low as compared to wrought Ti-6Al-4V because of the high hardness and brittle characteristics of additive manufactured titanium alloys
Purpose: The purpose of this paper is to study and compare the mechanical properties and machinability characteristics of additive manufactured titanium alloy Ti-6Al-4V with conventionally produced wrought titanium alloy,Ti-6Al-4V. The difference in mechanical properties such as yield strength, ultimate tensile strength, micro hardness, percentage of elongation and their effect on machinability characteristics like cutting forces and surface roughness are studied. It was found that higher strength and hardness of SLM Ti-6Al-4V compared to wrought Ti-6Al-4V owing to its peculiar acicular microstructure significantly affected the cutting forces and surface roughness. High cutting forces and low surface roughness were observed during machining of additive manufactured components compared to its wrought counterpart because of their difference in strength, hardness and ductility.Design/methodology/approach: Mechanical properties like yield strength, ultimate tensile strength, hardness and percentage of elongation and machinability characteristics like cutting forces and surface roughness were studied for both wrought and additive manufactured Ti-6Al-4V.Findings: Mechanical properties like yield strength, ultimate tensile strength and hardness were higher for additive manufactured components as compared to the wrought component. However additive manufactured components significantly lacked in ductility as compared to the wrought parts. Concerning machining, higher cutting forces and lower surface roughness were observed in additive manufactured Ti-6Al-4V compared to the wrought part as a result of differences in mechanical properties of these differently processed materials.Originality/value: This paper, for the first time, discusses the machining capabilities of additive manufactured Ti-6Al-4V.
Titanium alloys are of great demand in the aerospace and biomedical industries. Most the titanium products are either cast or sintered to required shape and finish machined to get the appropriate surface texture to meet the design requirements. Ti-6Al-4V is often referred as work horse among the titanium alloys due to its heavy use in the aerospace industry. This paper is an attempt to investigate and improve the machining performance of Ti-6Al-4V. Thin wall machining is an advance machining technique especially used in machining turbine blades which can be done both in a conventional way and using a special technique known as trochoidal milling. The experimental design consists of conducting trials using combination of cutting parameters such as cutting speed (vc), 90 and 120 m/min; feed/tooth (fz) of 0.25 and 0.35mm/min; step over (ae) 0.3 and 0.2; at constant depth of cut (ap) 20mm and using coolant. A preliminary assessment of machinability of Ti-6Al-4V during thin wall machining using trochoidal milling is done. A correlation established using cutting force, surface texture and dimensional accuracy
This research work presents a machinability study between wrought grade titanium and selective laser melted (SLM) titanium Ti-6Al-4V in a face turning operation, machined at cutting speeds between 60 and 180 m/min. Machinability characteristics such as tool wear, cutting forces, and machined surface quality were investigated. Coating delamination, adhesion, abrasion, attrition, and chipping wear mechanisms were dominant during machining of SLM Ti-6Al-4V. Maximum flank wear was found higher in machining SLM Ti-6Al-4V compared to wrought Ti-6Al-4V at all speeds. It was also found that high machining speeds lead to catastrophic failure of the cutting tool during machining of SLM Ti-6Al-4V. Cutting force was higher in machining SLM Ti-6Al-4V as compared to wrought Ti-6Al-4V for all cutting speeds due to its higher strength and hardness. Surface finish improved with the cutting speed despite the high tool wear observed at high machining speeds. Overall, machinability of SLM Ti-6Al-4V was found poor as compared to the wrought alloy.
28 August 2017 in Australian Journal of Mechanical Engineering
In this research work, chip formation characteristics of selective laser-melted (SLM) Ti–6Al–4V in both ‘as built’ and ‘heat treated’ conditions are studied and compared with conventional wrought Ti–6Al–4V. Machined chips and partially deformed chips were collected from turning trials and quick stop experiments to study the nature of chip formation characteristics. Chip formation studies reveal that, ‘segmented’ or ‘saw tooth’ chips were produced during machining of SLM Ti–6Al–4V materials. The tendency to form segmented chips was higher in SLM Ti–6Al–4V materials as compared to conventionally produced wrought Ti–6Al–4V. In addition, cracks were found to be a common feature in primary and secondary deformation zones of SLM Ti–6Al–4V chip samples, illustrating that periodic crack initiation is the root cause of ‘saw tooth’ formation during machining. Furthermore, the tendency to form build up edge during machining was less in SLM Ti–6Al–4V materials compared to wrought Ti–6Al–4V, influencing the machined surface finish.