Manikandakumar Shunmugavel

Manikandakumar Shunmugavel

Auto-generated profile, based on publicly available information

Manikandakumar Shunmugavel

School of Engineering, Deakin University, Geelong, Australia

Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
17 October 2017 in Rapid Prototyping Journal
Verified
Journal Article
Closed access
MSManikandakumar Shunmugavel
Manikandakumar Shunmugavel
APAshwin Polishetty
Ashwin Polishetty
MGMoshe Goldberg
Moshe Goldberg
RSRajkumar Singh
Rajkumar Singh
GLGuy Littlefair
Guy Littlefair
Purpose: The purpose of this paper is to study and compare the mechanical properties and machinability characteristics of additive manufactured titanium alloy Ti-6Al-4V with conventionally produced wrought titanium alloy,Ti-6Al-4V. The difference in mechanical properties such as yield strength, ultimate tensile strength, micro hardness, percentage of elongation and their effect on machinability characteristics like cutting forces and surface roughness are studied. It was found that higher strength and hardness of SLM Ti-6Al-4V compared to wrought Ti-6Al-4V owing to its peculiar acicular microstructure significantly affected the cutting forces and surface roughness. High cutting forces and low surface roughness were observed during machining of additive manufactured components compared to its wrought counterpart because of their difference in strength, hardness and ductility.Design/methodology/approach: Mechanical properties like yield strength, ultimate tensile strength, hardness and percentage of elongation and machinability characteristics like cutting forces and surface roughness were studied for both wrought and additive manufactured Ti-6Al-4V.Findings: Mechanical properties like yield strength, ultimate tensile strength and hardness were higher for additive manufactured components as compared to the wrought component. However additive manufactured components significantly lacked in ductility as compared to the wrought parts. Concerning machining, higher cutting forces and lower surface roughness were observed in additive manufactured Ti-6Al-4V compared to the wrought part as a result of differences in mechanical properties of these differently processed materials.Originality/value: This paper, for the first time, discusses the machining capabilities of additive manufactured Ti-6Al-4V.

1 August 2018 in Measurement
Verified
Journal Article
Closed access
JPJayakrishnan Unnikrishna Pillai
Jayakrishnan Unnikrishna Pillai
ISIkshit Sanghrajka
Ikshit Sanghrajka
MSManikandakumar Shunmugavel
Manikandakumar Shunmugavel
TMT. Muthuramalingam
T. Muthuramalingam
MGMoshe Goldberg
Moshe Goldberg
GLGuy Littlefair
Guy Littlefair

10 October 2016 in Journal of Metallurgy
Verified
Journal Article
Open access
PDF file
MSManikandakumar Shunmugavel
Manikandakumar Shunmugavel
APAshwin Polishetty
Ashwin Polishetty
JNJunior Nomani
Junior Nomani
MGMoshe Goldberg
Moshe Goldberg
GLGuy Littlefair
Guy Littlefair
This research work presents a machinability study between wrought grade titanium and selective laser melted (SLM) titanium Ti-6Al-4V in a face turning operation, machined at cutting speeds between 60 and 180 m/min. Machinability characteristics such as tool wear, cutting forces, and machined surface quality were investigated. Coating delamination, adhesion, abrasion, attrition, and chipping wear mechanisms were dominant during machining of SLM Ti-6Al-4V. Maximum flank wear was found higher in machining SLM Ti-6Al-4V compared to wrought Ti-6Al-4V at all speeds. It was also found that high machining speeds lead to catastrophic failure of the cutting tool during machining of SLM Ti-6Al-4V. Cutting force was higher in machining SLM Ti-6Al-4V as compared to wrought Ti-6Al-4V for all cutting speeds due to its higher strength and hardness. Surface finish improved with the cutting speed despite the high tool wear observed at high machining speeds. Overall, machinability of SLM Ti-6Al-4V was found poor as compared to the wrought alloy.

28 August 2017 in Australian Journal of Mechanical Engineering
Verified
Journal Article
Closed access
MSManikandakumar Shunmugavel
Manikandakumar Shunmugavel
MGMoshe Goldberg
Moshe Goldberg
APAshwin Polishetty
Ashwin Polishetty
JNJunior Nomani
Junior Nomani
Shoujin SunShoujin Sun
Shoujin Sun
GLGuy Littlefair
Guy Littlefair
In this research work, chip formation characteristics of selective laser-melted (SLM) Ti–6Al–4V in both ‘as built’ and ‘heat treated’ conditions are studied and compared with conventional wrought Ti–6Al–4V. Machined chips and partially deformed chips were collected from turning trials and quick stop experiments to study the nature of chip formation characteristics. Chip formation studies reveal that, ‘segmented’ or ‘saw tooth’ chips were produced during machining of SLM Ti–6Al–4V materials. The tendency to form segmented chips was higher in SLM Ti–6Al–4V materials as compared to conventionally produced wrought Ti–6Al–4V. In addition, cracks were found to be a common feature in primary and secondary deformation zones of SLM Ti–6Al–4V chip samples, illustrating that periodic crack initiation is the root cause of ‘saw tooth’ formation during machining. Furthermore, the tendency to form build up edge during machining was less in SLM Ti–6Al–4V materials compared to wrought Ti–6Al–4V, influencing the machined surface finish.

1 January 2017
Verified
Book Chapter
Closed access
MSManikandakumar Shunmugavel
Manikandakumar Shunmugavel
APAshwin Polishetty
Ashwin Polishetty
MGMoshe Goldberg
Moshe Goldberg
RSRajkumar Singh
Rajkumar Singh
GLGuy Littlefair
Guy Littlefair
In this study, the tool wear and surface integrity during machining of wrought and Selective Laser Melted (SLM) titanium alloy (after heat treatment) are studied. Face turning trails were carried out on both the materials at different cutting speeds of 60,120 and 180 m/min. Cutting tools and machined specimens collected are characterized using scanning electron microscope, surface profiler and optical microscope to study the tool wear, machined surface quality and machining induced microstructural alterations. It was found that high cutting speeds lead to rapid tool wear during machining of SLM Ti-6Al-4V materials. Rapid tool wear observed at high cutting speeds in machining SLM Ti-6Al-4V resulted in damaging the surface integrity by 1) Deposition of chip/work material on the machined surface giving rise to higher surface roughness and 2) Increasing the depth of plastic deformation on the machined sub surface.