Shape memory and magnetic properties of a Heusler polycrystalline alloy were investigated by differential scanning calorimetry, the sample extraction method, and the three-terminal capacitance method. A unique martensitic transformation from the ferromagnetic parent phase to the antiferromagneticlike martensite phase was detected and magnetic-field-induced “reverse” transition was confirmed in a high magnetic field. In addition, a large magnetic-field-induced shape recovery strain of about 1.0% was observed to accompany reverse martensitic transformation, and the metamagnetic shape memory effect, which was firstly reported in a Heusler single crystal, was confirmed in a polycrystalline specimen.
The phase stability and magnetic properties of the half-metal-type alloy system were investigated. It was found that the occurrence of two-phase separation is unavoidable in a concentration range of less than , leading to deviation of the saturation magnetic moments from the generalized Slater–Pauling line. The -type phase becomes stable in a concentration range of more than , where no half-metallic behaviors are present. Consequently, it is concluded that the most favorable concentration for applications to spintronic devices is located around in alloys having the -type phase.
In advanced applications such as aerospace and space exploration, materials must balance lightness, functionality and extreme thermal fluctuation resistance1,2. Shape-memory alloys show promise with strength, toughness and substantial strain recovery due to superelasticity, but maintaining low mass and effective operation at cryogenic temperatures is challenging3–6. We hereby introduce a new shape-memory alloy that adheres to these stringent criteria. Predominantly composed of Ti and Al with a chemical composition of Ti75.25Al20Cr4.75, this alloy is characterized by a low density (4.36 × 103 kg m−3) and a high specific strength (185 × 103 Pa m3 per kg) at room temperature, while showing excellent superelasticity. The superelasticity, owing to a reversible stress-induced phase transformation from an ordered body-centred cubic parent phase to an ordered orthorhombic martensite, allows for a recoverable strain exceeding 7%. This functionality persists across a broad range of temperatures, from deep cryogenic 4.2 K to above room temperature, arising from an unconventional temperature dependence of transformation stresses. Below a certain threshold during cooling, the critical transformation stress inversely correlates with temperature. We interpret this behaviour from the perspective of a temperature-dependent anomalous lattice instability of the parent phase. This alloy holds potential in everyday appliances requiring flexible strain accommodation, as well as components designed for extreme environmental conditions such as deep space and liquefied gases.
The concentration dependence of magnetic properties in the austenite phase of NiCoMnIn and NiCoMnSn Heusler alloys was systematically investigated by the magnetization measurements. The for alloys linearly increases with increasing the Co content and fixed Sn content. Although showing a concave curve for ternary alloys, the Sn content-dependence of magnetic moment per formula unit changes from the concave curve to a straight line when Co is substituted for Ni. On the other hand, the In content-dependence of the magnetic moment for alloys is perfectly linear as is that in the ternary alloys.
Martensitic transformation behaviors at low temperatures in polycrystalline Ti-51.8Ni (at. %) alloy were investigated with compressive stress. Superelasticity with almost complete shape recovery was confirmed at temperatures of 40–180 K. In stress-induced transformation at fixed temperatures, while the reverse transformation finishing stress monotonically decreased with decreasing test temperature, the forward transformation starting stress changed from decrease to increase at about 125 K. Forward and reverse transformation temperatures evaluated under constant stresses of 50 and 750 MPa were generally coincident with the results determined at the constant temperatures, where “heating-induced forward transformation” was confirmed under a stress of 750 MPa.