This study aims at analyzing the response of Li-ion cells and at identifying the hazards and governing phenomena from hard to soft external short circuit conditions. 10 Ah pouch cells and 4.5 mAh coin cells were short circuited while synchronized current, potential and temperature signals, audio, IR and visual video recordings were registered. The anode, cathode and separator harvested from the cells were characterized by Scanning Electron Microscopy, micro X-ray Computed Tomography and 3D-profilometry. The complex short circuit behavior obtained can be described by 3 regions: In the first region 274C-rate is observed which is mainly governed by the cell's double and diffusion layer discharge. In the second region, the current drops significantly to 50–60C-rate where mass transport becomes the current limiting factor. The maximum temperature (77–121 °C) is reached and cell rupture, venting and electrolyte leakage may occur. In the final, third region the current decline continues due to the decaying electromotive force. The normalized external/internal resistance ratio is found to be the main influential factor on current and hazards rather than the external resistance or the capacity of the cell. The implications on the relevance and fitness-for-purpose of external short circuit test in standards are outlined.JRC.C.1-Energy Storag
The Sustainability Assessment of Second Life Applications of Automotive Batteries (SASLAB) exploratory research project of the European Commission’s Joint Research Centre (JRC) aims at developing and applying a methodology to analyse the sustainability of deploying electrified vehicles (xEV) batteries in second use applications. A mapping of industrial demonstration and publicly-funded research projects in the area is presented, followed by an experimental assessment of the capacity and impedance change of lithium-ion cells during calendar and cycle ageing. Fresh cells and cells aged in the laboratory, as well as under real-world driving conditions, have been characterised to understand their application-specific remaining lifetime, beyond the 70% to 80% end-of-first-use criterion. For this purpose, pre-aged cells were examined under duty-cycles that resemble those of second use grid-scale applications.
12 November 2019 in Journal of the Electrochemical Society
The mechanical degradation of 18650 lithium ion cells is studied by X-ray computed tomography and is correlated to the electrochemical performance. A method for the geometrical analysis of electrodes by computer tomography is developed and applied to charged and discharged cells. As shown in earlier studies, the geometry of the jelly roll is inhomogeneous leading to mechanical stress during charge/discharge cycles. This effect leads to significant deformations of the jelly roll, which can be analyzed by computed tomography. The detailed analysis reveals that expansion of the anode takes place as expected during charging, but the degree of expansion depends on the position within the battery cell: the largest expansion during charging was found within the area of strongest deformations, whereas other areas without any expansion of the jelly roll were also observed. It is reasoned that the observed inhomogeneous expansion/contraction contribute significantly to cell degradation. The strong expansion within the deformed areas leads to sharp bending of the electrodes resulting in delamination of active layers. On the other hand, the absence of anode expansion reflected by a lack of increase in thickness when charging may indicate pore clogging assuming that the additional volume of graphite with intercalated lithium has to be accommodated within the pore structure.