In the as-cast state, Al–Mg–Si alloys are not suitable for hot forming. They present low ductility due to the presence of intermetallic β-AlFeSi particles that form in the interdendritic regions during the solidification process. Homogenization treatments promote the transformation of these particles into α-(FeMn)Si particles, which are smaller in size and more rounded in shape, thus improving the ductility of the material. This paper analyses the influence of various solution treatments on the transformation of β-AlFeSi particles into α-(FeMn)Si particles in an Al 6063 alloy. Their effect on different ageing treatments in the 150–180 °C temperature range is also studied. An increase in the solution temperature favours greater transformation of the β-AlFeSi particles into α-(FeMn)Si, dissolving a greater amount of Si, thereby having a significant effect on subsequent ageing. We found that as the dwell time at a temperature of 600 °C increases, the rate of dissolution of the Fe atoms from α-(FeMn)Si particles exceeds the rate of incorporation of Mn atoms into said particles. This seems to produce a delay in reaching the peak hardness values in ageing treatments, which warrants further research to model this behaviour. The optimal solution treatment takes place at around 600 °C and the highest obtained peak hardness value is 104 HV after a 2 h solution treatment at said temperature and ageing at 160 °C for 12 h.
With the aim of improving erosive wear resistance in hypoeutectic white cast irons with 18% Cr and 2% Mo, several samples of this grade were subjected to different heat treatments at 1000 °C to destabilize the austenite. The dwell times at this temperature varied from 4 to 24 h and the samples were cooled in air or oil. The existing phases were identified and quantified by applying the Rietveld structural refinement method. The results were correlated with the hardness of the material and with the microhardness of the matrix constituent. The greatest resistance to erosive wear was achieved in those samples that had a higher percentage of secondary carbides. The longer the dwell time at the destabilization temperature of austenite, the greater the amount of precipitated secondary carbides. However, the percentage of dissolved eutectic carbides is also higher. These eutectic carbides were formed as a result of non-equilibrium solidification. Low cooling rates (in still air) can offset this solution of eutectic carbides via the additional precipitation of secondary carbides in the 600–400 °C temperature range. A sharp decrease is observed in the percentage of retained austenite in those treatments with dwell times at 1000 °C equal to or greater than 12 h, reaching minimum values of around 2% volume. The percentage of retained austenite was always lower after oil quenching and the hardness of oil quenched samples was observed to be greater than those quenched in air. In these samples, the maximum hardness value obtained was 993 HV after a 12 h dwell, which result from the optimum balance between the percentages of retained austenite and of precipitated carbides.
15 December 2007 in Journal of Materials Processing Technology
Vanadis 10 steel is a powder metallurgy (PM) processed tool steel. It is a ledeburitic steel with 8% Cr and 10% V. By deliberately varying the process parameters related to the quenching, tempering, and nitriding of these steels, the aim of this study is to determine which of these parameters have a significant influence on its adhesive wear resistance. The research methodology employed was a Design of Experiments (DoE) with six factors and two levels for each factor. The tempering temperature, number of temperings, and carrying out of a thermochemical nitriding treatment were found to have a significant effect. To increase adhesive wear resistance, austenitization at 1100 °C with air cooling is recommended, followed by three temperings at 500 °C and a subsequent nitriding treatment. It should be noted that the quench cooling medium does not have a significant influence on wear resistance. Furthermore, (Fe,Cr)7C3 (M7C3 carbides) are transformed into carbonitrides during nitriding. However, (Fe,V)C (MC carbides) are not affected by this nitriding process.
High-Cr hypo-eutectic white cast irons are used in very demanding environments that require high resistance to erosive wear. The influence on the microstructural variation and erosive wear resistance of several fundamental factors related to the thermal treatments of these cast irons was analysed by means of a fractional Design of Experiments (DoE). These factors included the ones related to the destabilization of austenite. The precipitated phases were identified by X-ray diffraction (XRD), while the Rietveld structural refinement method was used to determine their percentages by weight. Erosion wear resistance was calculated using the test defined by ASTM G76. It was concluded that the quench cooling medium does not significantly influence either erosive wear resistance or the proportion of martensite or retained austenite. The destabilization temperature is a key factor with respect to the percentage of retained austenite. In order to increase the amount of martensite and decrease the amount of retained austenite, temperatures not exceeding 1000 °C are required. An increase of 100 °C in the destabilization temperature can lead to a 25% increase in retained austenite. Moreover, tempering temperatures of around 500 °C favour an additional increase in the percentage of martensite. Erosive wear commences on the matrix constituent without initially affecting the eutectic carbides. Once the deterioration of the matrix constituent surrounding these carbides occurs, they are released. High tempering times provide an increase in resistance to erosive wear due to a second destabilization of austenite during the said tempering.
Hypoeutectic white cast irons with a high chrome content are commonly used in the industrial mining sector where there is a demand for both high resistance to adhesive wear and an acceptable toughness for the absorption of impacts and falls of diverse materials. Through the application of a design of experiment (DoE) technique, factors related to thermal treatment are analyzed with respect to resistance to sliding wear, maximum rupture stress and toughness. The results show that, in order to increase resistance to adhesive wear, it is convenient to use destabilization temperatures of 1050 °C and tempering of two hours at 400 °C. This foments a very hard martensite and a high proportion of highly alloyed retained austenite, which, with low tempering, achieves a precipitation of carbides from this austenite with hardly any loss of hardness of the martensite. In order to increase the energy which this material is capable of absorbing until breakage, furnace cooling set at 150 °C followed by tempering at 550 °C would be favorable. Slower cooling implies a greater quantity of conditioned retained austenite, so that, following this, it may be transformed into lower bainite with a high density of finely dispersed precipitated carbides. Furthermore, this tempering also allows the transformation of martensite into ferrite with finely dispersed carbides.