Acid leaching is an effective method for dephosphorization; however, it is time-consuming and requires a high amount of acid consumption, resulting in increased production costs and environmental risks. This work aims to remove silicon, aluminum, and phosphorus from high-phosphorus oolitic magnetite concentrate through high-pressure alkaline leaching and ultrasonic acid leaching. Compared with traditional acid leaching processes, the sulfuric acid dosage can be significantly reduced from 200 kg/t to 100 kg/t, and the pickling time is shortened from 60 min to 10 min. Thermodynamic and kinetic studies have demonstrated that acid leaching facilitates apatite dissolution at low temperatures, whereas the dephosphorization reaction is controlled mainly by diffusion. The application of ultrasonic waves leads to finer particle sizes and greatly increased specific surface areas, thereby accelerating the diffusion rate of the leaching agent. Furthermore, microscopic analysis revealed that under the influence of ultrasonic waves, numerous micro-fragments and pores form on particle surfaces due to cavitation effects and mechanical forces generated by ultrasonic waves. These factors promote both the reaction rates and diffusion processes of the leaching agent while enhancing the overall leaching efficiency.
Diverging from conventional dephosphorization approaches, this study employs a novel pre-reduction and smelting separation (PR-SS) to efficiently co-recover iron and phosphorus from high-phosphorus oolitic iron ore, directly yielding Fe–P alloy, and the Fe–P alloy shows potential as feedstock for high-phosphorus weathering steel or wear-resistant cast iron, indicating promising application prospects. Using oolitic magnetite concentrate (52.06% Fe, 0.37% P) as feedstock, optimized conditions including pre-reduction at 1050 °C for 2 h with C/Fe mass ratio of 2, followed by smelting separation at 1550 °C for 20 min with 5% coke, produced a metallic phase containing 99.24% Fe and 0.73% P. Iron and phosphorus recoveries reached 99.73% and 99.15%, respectively. EPMA microanalysis confirmed spatial correlation between iron and phosphorus in the metallic phase, with undetectable phosphorus signals in vitreous slag. This evidence suggests preferential phosphorus enrichment through interfacial mass transfer along the pathway of the slag phase to the metal interface and finally the iron matrix, forming homogeneous Fe–P solid solutions. The phosphorus migration mechanism involves sequential stages: apatite lattice decomposition liberates reactive P2O5 under SiO2/Al2O3 influence; slag–iron interfacial co-reduction generates Fe3P intermediates; Fe3P incorporation into the iron matrix establishes stable solid solutions.
6 July 2025 in Asia-Pacific Journal of Chemical Engineering
High-phosphorus oolitic iron ores (HPOIOs) possess abundant reserves but are incompatible with conventional blast furnace ironmaking, as phosphorus migrates into hot metals during carbothermic reduction, preventing the production of low-phosphorus clean steel. To overcome this limitation, an innovative approach integrating alkaline briquette direct reduction and smelting separation was proposed. Briquettes were prepared from oolitic magnetite concentrate (52.01 wt% Fe, 0.29 wt% P, 0.11 wt% S) with a basicity (R) of 2.0 and 5 wt% MgO added as a desulfurizer. After direct reduction and smelting separation, the resulting metallic iron exhibited a content of 98.56 wt% Fe, with 0.036 wt% P and 0.046 wt% S, achieving an Fe recovery of 87.63%. The dephosphorization and desulfurization efficiencies reached 94.67% and 90.56%, respectively, meeting the clean steel requirements. Phosphorus was effectively stabilized within the gehlenite and merwinite phases as a solid solution of Ca3(PO4)2, inhibiting its transfer to iron. Thermodynamic analyses confirmed that high basicity (R ≥ 2.0) significantly suppressed P2O5 activity, preventing phosphate reduction. The formation of a Ca3(PO4)2–Ca2SiO4 solid solution further obstructed phosphorus migration. This dual mechanism of “chemical fixation and thermodynamic stabilization” enables efficient dephosphorization, offering a sustainable pathway for utilizing HPOIOs.
The sintering process represents a primary source of dust, SO2, NOx, and CO2 emissions in steel mills. Utilizing high-grade concentrate with low impurity content can directly reduce slag generation at the source, thereby decreasing fuel consumption and minimizing associated emissions. This study investigated the physicochemical properties, microstructure, and elemental distribution of hematite concentrates (H2 and H3) and H1 sinter fines. Sinter pot tests were conducted to evaluate the effects of blending these two concentrates on sintering performance and key quality indices. Microstructural analysis and quantitative phase composition statistics of the sintered products were performed to elucidate the mechanisms by which these concentrates influence sintering outcomes. Results demonstrated that replacing 33% H1 sinter fines with 33% H2 or H3 concentrates reduced the tumbler index from 73.6% to 68.5% and 73.2%, respectively. The productivity coefficient decreased to 68.5% and 73.2%, while solid fuel consumption increased from 73.9 kg/t to 90.5 kg/t and 81.2 kg/t. RI declined from 80.0% to 77.9% and 78.4%, whereas RDI improved from 72.9% to 76.8% and 75.8%.