To investigate hydrogen absorption behavior into carbon steel during corrosion in an aqueous sodium chloride (NaCl) droplet, a simultaneous measurement system of the corrosion potential, Ecorr and hydrogen permeation current, iper was developed using the Kelvin probe (KP) technique and the Devanathan–Stachurski (DS) method, respectively. This system outputs the interrelation between corrosion and hydrogen absorption into steel throughout the drying process of an NaCl droplet. Our results showed that hydrogen absorption into the steel occurred when the Ecorr shifted in less noble direction under wet conditions, and ceased at a higher potential of Ecorr when the steel surface dried up. Based on the results of the transients of the iper, the amount of hydrogen absorbed during the drying of the NaCl droplet increased with NaCl concentration, which was attributed to the negative shift of the Ecorr. Furthermore, the amount of hydrogen absorbed within one wet-dry cycle changed with the number of cycles, due to the expansion of the corroded area and the formation of iron rust.
2 June 2018 in Journal of the Electrochemical Society
Zinc corrosion under 0.2 M NaCl solution films 5–800 μm in thickness was studied by electrochemical impedance spectroscopy (EIS). As-polished and rusted zinc plates obtained by exposure to a natural atmospheric environment for 1, 3, 6, and 12 months were used as working electrodes. The obtained EIS results were analyzed using a transmission line equivalent circuit to determine the charge transfer resistance (Rct), the reciprocal of which is proportional to the corrosion current density. For the as-polished zinc, the corrosion behavior is divided into three regions by the solution film thickness (Xf). In Region I (Xf: 800–200 μm), Rct−1 is independent of Xf and is approximately ten times smaller than that for carbon steel. In Region II (Xf: 200–25 μm), however, Rct−1 increases with decreasing solution thickness down to approximately 25 μm due to an enhancement of the oxygen diffusion (cathodic process) through the solution film. In Region III (Xf < 25 μm), further decreases in thickness reduce Rct−1 because the zinc dissolution (anodic process) is suppressed. In contrast, Rct−1 of the rusted zinc is independent of Xf because the charge transfer process is strongly suppressed by the zinc corrosion products, which were identified as simonkolleite and zinc oxide.
10 June 2019 in Journal of the Electrochemical Society
In this study, we investigated the hydrogen absorption behavior of pre-rusted steel in an NaCl droplet by measuring the hydrogen permeation current and corrosion potential. To prepare the pre-rusted steel, a 30-μL droplet of a 0.1-mol/dm3 NaCl solution was placed on the surface of steel and exposed to wet-dry cyclic conditions by changing the relative humidity (RH) repeatedly from 40% to 95% at a constant rate of 27.5%/h and 298 K. The hydrogen permeation current and corrosion potential of the pre-rusted steel were measured during the drying of an electrolyte droplet using an electrochemical hydrogen permeation test and the Kelvin probe (KP) technique, respectively. The corrosion potential of the pre-rusted steel shifted in the negative direction simultaneous with the evolution of the hydrogen permeation current during the drying of the droplet. The hydrogen permeation current increased with the number of wet-dry cycles in the early stages of the rusting process, which related to the negative shift in corrosion potential. As the whole surface of the steel was covered with iron rust in the later stages of the rusting process, the corrosion potential shifted in the positive direction and the hydrogen absorption current decreased gradually.
We studied the passivation behavior of hot-dip galvanized steel (HDG) rebar and ordinary steel (black) rebar in fresh concrete using electrochemical techniques. Although the passivation behavior was considerably different, both types of rebar were fully passivated. The black rebar was immediately passivated after exposure to fresh concrete; however, the HDG rebar was passivated after being kept active for tens of hours. The corrosion rates of both types of rebars after passivation seemed comparable. To further investigate the difference, we monitored the passivation processes by electrochemical impedance spectroscopy using carbon steel and zinc electrodes in fresh mortar and saturated Ca(OH)2 solution, which simulated the water in the concrete pores; furthermore, we observed similar trends for fresh concrete. Initially, the Zn surface was partially covered with calcium hydroxy zincate (CHZ) whose coverage increased with exposure time. Finally, the surface was fully covered with a CHZ film after passivation.