Wurtzite AlN is an ultrawide bandgap semiconductor that has been developed for applications including power electronics and optoelectronics. Thermal management of these applications is the key for stable device performance and allowing for long lifetimes. However, the intrinsic high thermal conductivity of bulk AlN predicted by theoretical calculations has not been experimentally observed because of the difficulty in producing high-quality materials. This work reports the growth of thick (>15 μm) AlN layers by metal-organic chemical vapor deposition and experimental observation of intrinsic thermal conductivity from 130 to 480 K that matches density-functional-theory calculations for single crystal AlN, producing some of the highest values ever measured. Detailed material characterizations confirm the high quality of these AlN samples with one or two orders of magnitude lower impurity concentrations than commercially available bulk AlN. The thermal conductivity of these commercially available bulk AlN substrates are also measured as comparison. To interpret the reduced thermal conductivity, a simple Callaway model is built. This work demonstrates the possibility of obtaining theoretically high values of thermal conductivity in AlN and will impact the thermal management and reliability of future electronic and optoelectronics devices.
Conventional epitaxy of semiconductor films requires a compatible single crystalline substrate and precisely controlled growth conditions, which limit the price competitiveness and versatility of the process. We demonstrate substrate-tolerant nano-heteroepitaxy (NHE) of high-quality formamidinium-lead-tri-iodide (FAPbI3) perovskite films. The layered perovskite templates the solid-state phase conversion of FAPbI3 from its hexagonal non-perovskite phase to the cubic perovskite polymorph, where the growth kinetics are controlled by a synergistic effect between strain and entropy. The slow heteroepitaxial crystal growth enlarged the perovskite crystals by 10-fold with a reduced defect density and strong preferred orientation. This NHE is readily applicable to various substrates used for devices. The proof-of-concept solar cell and light-emitting diode devices based on the NHE-FAPbI3 showed efficiencies and stabilities superior to those of devices fabricated without NHE.
A unified fundamental understanding of interfacial thermal transport is missing due to the complicated nature of interfaces. Because of the difficulty to grow high-quality interfaces and lack of materials characterization, the experimentally measured thermal boundary conductance (TBC) in the literature are usually not the same as the ideally modelled interfaces. This work provides a systematic study of TBC across the highest-quality (atomically sharp, harmonic-matched, and ultraclean) epitaxial (111) Al||(0001) sapphire interfaces to date. The comparison of measured high TBC with theoretical models shows that elastic phonon transport dominates the interfacial thermal transport and other mechanisms play negligible roles. This is confirmed by a nearly constant transmission coefficient by scaling the TBC with the Al heat capacity and sapphire heat capacity with phonon frequency lower than 10 THz. Finally, the findings in this work will impact applications such as electronics thermal management, thermoelectric energy conversion, and battery safety.
The coefficients of thermal expansion (CTEs) of single crystalline, monoclinic β-Ga2O3 were determined by employing high-resolution X-ray diffraction measurements. This work reports the CTE measurements on a single crystalline β-Ga2O3 substrate. The CTE values along the “a,” “b,” and “c” axes are 3.77 × 10−6 °C−1, 7.80 × 10−6 °C−1, and 6.34 × 10−6 °C−1, respectively, and the CTE of the angle β (the angle between the “a” and “c” axes) is determined to be 1.31 × 10−4 ° K−1. All CTE values reported here are linear under the temperature regime between room temperature and 1000 °C. All measurements were performed in a controlled nitrogen gas environment, and no surface degradation was observed after these measurements. Thermal strain calculations with different material combinations involving β-Ga2O3 are also presented relevant to both epitaxial and wafer bonding applications for Si, InP, 3C–SiC, 6H–SiC, GaN, and sapphire.
We report on high-quality n-Al0.87Ga0.13N-A0.64Ga0.36N heterostructures over single crystal AlN. For these pseudomorphic heterostructures, high-resolution X-ray and X-ray Topographic analysis was used to establish a threading dislocation density of 7 × 103 cm−2. Using reverse composition graded n+-AlxGa1-xN contact layers, we obtained linear ohmic contacts with 4.3 Ω mm specific resistance. A critical breakdown field >11 MV cm−1 was also measured. In combination with the channel resistance of 2400 Ω sq−1, these translate to a Baliga’s Figure of Merit of 2.27 GW cm−2. This, to the best of our knowledge is the highest reported value for extreme bandgap AlGaN heterostructures.
1 January 2023 in Journal of Vacuum Science & Technology A
Smooth (< 0.5 nm rms) and subsurface damage-free (010) β-Ga2O3 was achieved with low-pressure chemical mechanical polishing. An applied pressure of 1 kPa along with colloidal silica and poromeric polyurethane polishing pads rotating at 30 rpm was found to be the optimal polishing parameters for (010) β-Ga2O3. Using higher pressures typically employed in the current literature induced subsurface damage in the substrates. Diffuse scatter intensity of triple-axis x-ray rocking curves was used to determine the presence of subsurface lattice damage, which was quantified by measuring peak widths below the half maximum (i.e., FWXM where X < 0.5). The initially rough surfaces of (010) β-Ga2O3 substrates due to wafer slicing and grinding were lapped and polished. A 5 μm Al2O3 slurry followed by a 0.3 μm Al2O3 slurry was used as the primary lap material removal step. The material removal rates were ∼20 and ∼9 μm/h, respectively. Then, chemical mechanical polishing was performed using colloidal alumina followed by colloidal silica. The removal rates were ∼1.3 and ∼0.4 μm/h, respectively. Only colloidal silica showed the complete removal of subsurface damage. The final (020) β-Ga2O3 rocking curve FWHM was ∼13″ and FW(0.001)M was ∼120″, which matches the widths of commercially available pristine (010) β-Ga2O3. A final cleaning step using dilute bleach and dilute citric acid to remove residual silica slurry particles from the surface was demonstrated.