In the domain of new energy vehicles, the control of welding deformation in aluminum alloy battery systems poses substantial challenges. The existing methodologies for diminishing welding deformation, such as laser segmented skip welding, alteration of welding path sequences, numerical simulation prediction, and post-weld heat treatment, still possess room for further optimization when applied to intricate welding structures. In this research, a novel adjustable-ring-mode laser in conjunction with the oscillation welding technique was employed to explore the impacts of fiber core diameter, laser light field brightness distribution, and process parameters on weld formation. The regulation of welding deformation was achieved through optimizing the welding process and adjusting the welding path. The results indicate that when the fiber core diameter is 50/150 µm and the light field brightness distribution is H, the weld size exhibits the highest stability. Under the conditions of process parameters p = 5300 W, v = 5.4 m/min, A = 1.6 mm, f = 120 Hz, and θ = 40°, and with the spot position located at the bottom of the side of the upper substrate, the optimal weld formation is obtained. After optimizing the welding path, the maximum Z-direction deformation of the weld is 1.403 mm, representing a reduction of 1.702 mm compared to the previous value. This work is capable of providing novel theoretical guidance and technical insights for the control of welding deformation in thin aluminum alloy plates.
Wire arc additive manufacturing technology with cold metal transfer and pulse welding (CMT+P) is a promising technology for fabricating complex metal structures. In this paper, a lot of basic research was conducted on the corner-constrained and unconstrained zones of 4043 aluminum alloy made using CMT+P. In particular, the microstructure morphology and mechanical properties of the corner-constrained and unconstrained zones of 4043 aluminum alloy made by CMT+P were studied by using a thermal field emission scanning electron microscope, a microhardness tester, etc. The results showed that there were cellular crystals at the top, columnar dendritic crystals in the middle and bottom, and smaller equiaxed crystals in the bottom center. The grain size in the corner-constrained zone was larger than that in the unconstrained zone, and the grain size increased by about 88.34%. Moreover, the microhardness of the unconstrained zone was 50 HV, while the microhardness of the corner-constrained zone was 45 HV. Furthermore, the tensile strength of this material was 148 MPa, the elongation was 31%, the fracture behavior in the middle and top areas was typical of a ductile fracture, and the fracture in the bottom area was a mixed ductile–brittle fracture dominated by the ductile fracture.
During underwater laser welding, the coupling among water cooling, gas–liquid interface disturbances, and metal-vapor recoil pressure means that the relationships among plasma evolution, the thermal state of the keyhole, and spatter behavior remain insufficiently understood. In this study, 304NG stainless steel was welded in air and under local dry underwater conditions using a 10 kW continuous-wave fiber laser with a wavelength of 1070 nm to investigate the effects of laser power on the energy state and process stability of underwater welding. The underwater experiments were conducted in deionized water, with the workpiece positioned approximately 100 mm below the free water surface and without additional pressurization. High-speed imaging, infrared thermography, and spectroscopy were employed to characterize the transient evolution of the plasma and spatter, the apparent thermal state near the keyhole opening, and the spectral characteristics of the underwater plasma, respectively, while the plasma excitation temperature was calculated using the Boltzmann multi-line fitting method. The results showed that as the laser power increased from 2000 to 4000 W, the plasma size and temporal persistence increased significantly in both air and underwater environments; the transverse width of the underwater plasma at T0 + 0.8 ms increased from approximately 2.7 to 5.8 mm, while the average maximum apparent temperature near the keyhole opening increased from approximately 2477 to 3071 °C. Meanwhile, the intensities of the characteristic Fe I lines increased overall, and the plasma excitation temperature increased from 5977 to 6510 K, consistent with the expansion of the plasma-emitting region, the enhanced persistence of the high-temperature core, and the increase in the apparent temperature near the keyhole opening. This study aims to provide a new systematic understanding and technical insights into plasma evolution during underwater laser welding.