With surging demand for lightweight, high-strength metal components in high-end equipment and large-scale engineering structures, additive manufacturing of low-alloy ultra-high-strength steel (LUHSS) has become a hot research topic. Wire arc additive manufacturing (WAAM) shows remarkable potential for fabricating large LUHSS components; however, repetitive thermal cycles can trigger in situ tempering, significantly affecting carbide evolution and mechanical properties. To address this, this study employed a cold metal transfer plus pulse (CMT+P)-based WAAM process to fabricate thin-walled LUHSS specimens under gradient heat input conditions (3.73, 7.37, and 11.8 kJ/cm) and systematically characterized their mechanical properties and microstructure. The results indicate that increasing heat input enlarges the melt pool and weld bead dimensions, while excessive heat input exacerbates oxide inclusion precipitation and compromises forming quality; the deposited microstructure consists primarily of lamellar martensite, retained austenite, and dispersed carbides. Heat input can precisely control the in situ tempering effect, driving the gradual transformation of carbides from pure Cr23C6 to a coexistence of Cr23C6 and Cr3C, ultimately forming Cr7C3. Grain coarsening and dislocation recovery weaken the material’s strengthening effect. At a heat input of 3.73 kJ/cm, the specimen exhibited excellent strength–ductility synergy and near-isotropic characteristics, with tensile strength, yield strength, and elongation of 1,529 MPa, 1,272 MPa, and 12.3%, respectively. This study shows how heat input-induced in situ tempering regulates precipitation behavior and the mechanical properties of WAAM-formed LUHSS.
Surface remelting is an effective method for modifying surface microstructures and improving the mechanical properties of metallic materials. However, the influence of an underwater environment on the laser remelting behaviour of zirconium alloys remains insufficiently understood. In this study, commercially pure Zr60702 was subjected to laser surface remelting in air and underwater environments under identical processing parameters. The phase constitution, microstructure, microhardness, and wear resistance of the remelted samples were systematically investigated. The maximum remelting depth decreased from 507.08 μm in air to 191.35 μm underwater because of the enhanced heat extraction and reduced effective laser-energy input in the aqueous environment. Both remelted samples were dominated by α-Zr at room temperature, while underwater remelting produced finer acicular α′-Zr and refined Widmanstätten structures. The maximum hardness values of the underwater- and air-remelted samples reached 636.7 and 546.5 HV, respectively, compared with 198.3 HV for the base material. The wear volumes of the base material, air-remelted sample, and underwater-remelted sample were 7.04 × 107, 6.77 × 107, and 5.66 × 107 μm3, respectively. The improved wear resistance of the underwater-remelted sample was attributed to its refined microstructure and increased hardness, which suppressed plastic deformation and ploughing during sliding. These results demonstrate that underwater laser remelting is a promising method for improving the surface properties of Zr60702.
During underwater laser welding, the coupling among water cooling, gas–liquid interface disturbances, and metal-vapor recoil pressure means that the relationships among plasma evolution, the thermal state of the keyhole, and spatter behavior remain insufficiently understood. In this study, 304NG stainless steel was welded in air and under local dry underwater conditions using a 10 kW continuous-wave fiber laser with a wavelength of 1070 nm to investigate the effects of laser power on the energy state and process stability of underwater welding. The underwater experiments were conducted in deionized water, with the workpiece positioned approximately 100 mm below the free water surface and without additional pressurization. High-speed imaging, infrared thermography, and spectroscopy were employed to characterize the transient evolution of the plasma and spatter, the apparent thermal state near the keyhole opening, and the spectral characteristics of the underwater plasma, respectively, while the plasma excitation temperature was calculated using the Boltzmann multi-line fitting method. The results showed that as the laser power increased from 2000 to 4000 W, the plasma size and temporal persistence increased significantly in both air and underwater environments; the transverse width of the underwater plasma at T0 + 0.8 ms increased from approximately 2.7 to 5.8 mm, while the average maximum apparent temperature near the keyhole opening increased from approximately 2477 to 3071 °C. Meanwhile, the intensities of the characteristic Fe I lines increased overall, and the plasma excitation temperature increased from 5977 to 6510 K, consistent with the expansion of the plasma-emitting region, the enhanced persistence of the high-temperature core, and the increase in the apparent temperature near the keyhole opening. This study aims to provide a new systematic understanding and technical insights into plasma evolution during underwater laser welding.