Screen-printed electrochemical sensing platforms, due to their scales of economy and high reproducibility, can provide a useful approach to translate laboratory-based electrochemistry into the field. An important factor when utilising screen-printed electrodes (SPEs) is the determination of their real electrochemical surface area, which allows for the benchmarking of these SPEs and is an important parameter in quality control. In this paper, we consider the use of cyclic voltammetry and chronocoulometry to allow for the determination of the real electrochemical area of screen-printed electrochemical sensing platforms, highlighting to experimentalists the various parameters that need to be diligently considered and controlled in order to obtain useful measurements of the real electroactive area.
2D hexagonal boron nitride (2D-hBN) is a lesser utilised material than other 2D counterparts in electrochemistry due to initial reports of it being non-conductive. As we will demonstrate in this review, this common misconception is being challenged, and researchers are starting to utilise 2D-hBN in the field of electrochemistry, particularly as the basis of electroanalytical sensing platforms. In this critical review, we overview the use of 2D-hBN as an electroanalytical sensing platform summarising recent developments and trends and highlight future developments of this interesting, often overlooked, 2D material.
Herein, we report the fabrication and application of Li‐ion anodes for utilisation within Li‐ion batteries, which are fabricated via additive manufacturing/3D printing (fused deposition modelling) using a bespoke graphene/polylactic acid (PLA) filament, where the graphene content can be readily tailored and controlled over the range 1–40 wt. %. We demonstrate that a graphene content of 20 wt. % exhibits sufficient conductivity and critically, effective 3D printability for the rapid manufacturing of 3D printed freestanding anodes (3DAs); simplifying the components of the Li‐ion battery negating the need for a copper current collector. The 3DAs are physicochemically and electrochemically characterised and possess sufficient conductivity for electrochemical studies. Critically, it is found that if the 3DAs are used in Li‐ion batteries the specific capacity is very poor but can be significantly improved through the use of a chemical pre‐treatment. Such treatment induces an increased porosity, which results in a 200‐fold increase (after anode stabilisation) of the specific capacity (ca. 500 mAh g−1 at a current density of 40 mA g−1). This work significantly enhances the field of additive manufacturing/3D printed graphene based energy storage devices demonstrating that useful 3D printable batteries can be realised.
7 June 2023 in ACS Sustainable Chemistry & Engineering
Recycling used mixed material additively manufactured electroanalytical sensors into new 3D-printing filaments (both conductive and non-conductive) for the production of new sensors is reported herein. Additively manufactured (3D-printed) sensing platforms were transformed into a non-conductive filament for fused filament fabrication through four different methodologies (granulation, ball-milling, solvent mixing, and thermal mixing) with thermal mixing producing the best quality filament, as evidenced by the improved dispersion of fillers throughout the composite. Utilizing this thermal mixing methodology, and without supplementation with the virgin polymer, the filament was able to be cycled twice before failure. This was then used to process old sensors into an electrically conductive filament through the addition of carbon black into the thermal mixing process. Both recycled filaments (conductive and non-conductive) were utilized to produce a new electroanalytical sensing platform, which was tested for the cell's original application of acetaminophen determination. The fully recycled cell matched the electrochemical and electroanalytical performance of the original sensing platform, achieving a sensitivity of 22.4 ± 0.2 μA μM-1, a limit of detection of 3.2 ± 0.8 μM, and a recovery value of 95 ± 5% when tested using a real pharmaceutical sample. This study represents a paradigm shift in how sustainability and recycling can be utilized within additively manufactured electrochemistry toward promoting circular economy electrochemistry.