Comprehending the synergistic of surface treatments and oral environmental factors is paramount for optimizing the performance of 3D-printed dentures. This study evaluates flexural strength, hardness, roughness, and color stability of 3D-printed resins after two surface treatments and coffee thermocycling, to establish alternative polishing efficacy. Rectangular test specimens (64 × 10 × 3.3 ± 0.2 mm) were fabricated from a conventional heat-cured denture base material (Probase HC, n = 20) and four 3D-printed denture base materials (Nextdent; ND, Formlabs; FL, Senertek; ST, Powerresin; PR, n = 40 per group), resulting in a total sample size of N = 180. Specimens were randomly assigned to undergo either mechanical polishing or glazing, followed by 5000 cycles of coffee thermocycling (CTC). Color change (ΔE00) and surface roughness (Ra) were assessed both prior to and subsequent to CTC. Subsequently, the specimens were subjected to a 3-point bending test and a Vickers microhardness (VH) test. Statistical analysis of the data was performed using descriptive and analytical methods, with a significance level set at α = 0.05. The application of Vita Akzent® LC (VA) as a glaze material, while conferring supplementary protection against surface degradation during coffee thermocycling (CTC), resulted in a statistically significant increase in the initial surface roughness (Ra) values across all experimental 3D-printed groups (p < 0.05). It reduced the ΔE value of the FL group (p = 0.036) but did not have a statistically significant impact on the ΔE00 of other 3D-printed groups (p˃0.05). Additionally, VA enhanced the VH of most 3D-printed groups (p < 0.05). It improved the flexural strength of the PR and ST groups but decreased it for the FL group and had no significant effect on the ND group (p = 0.088). The mechanically polished specimens demonstrated acceptable Ra, ΔE00, and flexural strength values. However, they showed a lower VH than the glazed specimens. Glaze application resulted in improved mechanical strength and hardness for the majority of 3D-printed groups; however, its capacity to effectively reduce surface roughness and discoloration was consistently limited. Conversely, mechanical polishing maintained its beneficial effects, demonstrating clinically acceptable values across all assessed parameters. Therefore, comprehensive additional investigations are necessitated to fully elucidate the performance characteristics of glaze materials and their interactions with 3D-printed denture base materials.

29 October 2025 in BMC Oral Health
Verified
Journal Article
Open access
PDF file
EİEymen İzzettinoğlu
Eymen İzzettinoğlu
EEErdal Eroglu
Erdal Eroglu
High water sorption and solubility in total denture base materials are primary factors contributing to prosthetic failure, as they compromise both mechanical and aesthetic properties. This study investigated how three distinct surface treatments, varying aging protocols, and different curing parameters collectively influence the water sorption (Wsp) and solubility (Wsl) of 3D-printed denture base materials. This study evaluated the water sorption and solubility of 420 disc-shaped specimens (Ø15 × 2 ± 0,2 mm) fabricated from one conventional heat-cured acrylic resin (Probase; HC), one CAD-CAM Prepolymerized PMMA block (Bilkim; M), and one 3D-printed denture base material (Formlabs; 3DP ). All groups underwent three distinct surface treatments (mechanical polishing, Optiglaze, or Vita Akzent Glaze). The 3D-printed specimens were additionally subjected to four curing durations (10, 15, 30, 60 min) and two curing atmospheres (air and glycerin). Water sorption (Wsp) and solubility (Wsl) were assessed after three distinct aging protocols: 7 days of immersion in distilled water (Wsp-DW and Wsl-DW), 6 days of immersion in a denture cleaner (Wsp-DC and Wsl-DC), and 2000 thermocycles (Wsp-TC and Wsl-TC). Statistical analysis was conducted using non-parametric tests, as the Kolmogorov-Smirnov test revealed that the data were not normally distributed (p < 0.05). The Mann-Whitney U test was applied for comparisons between two categorical variables, while the Kruskal-Wallis test was used for three or more categories. For related groups, the Friedman test was employed. Pairwise comparisons were performed to identify specific differences among groups. All statistical analyses were conducted with significance levels set at α = 0.05 and 0.01. This study demonstrates that both manufacturing technology and surface treatment significantly influence the water sorption and solubility of dental acrylics. Conventional heat-polymerized acrylics exhibited the highest water sorption, whereas 3D-printed materials consistently showed the lowest (p < 0.01). Regarding solubility, heat-cured materials generally displayed the lowest values. Conversely, 3D-printed materials had the highest Wsl-DW and Wsl-TC, but the lowest Wsl-DC (p < 0.01). Glaze application effectively reduced both water sorption and solubility across all groups compared to mechanical polishing. Lastly, while glycerin curing of 3D-printed resins led to higher sorption but lower solubility, curing duration generally had no significant impact, with some 10-minute cured groups occasionally showing higher solubility (p < 0.01). All 3D-printed groups, irrespective of surface treatment or curing parameters, demonstrated water sorption (Wsp) and solubility (Wsl) values within the limits defined by ISO 4049 − 2019 (Wsp < 40 µg/mm³; Wsl < 7.5 µg/mm³). While glaze application effectively reduces these properties, adequate curing time and the use of a glycerin curing medium can similarly diminish solubility. However, curing duration was not found to have a statistically significant impact on water sorption.