The experiments were divided into two groups to establish a drying shrinkage model suitable for modified ceramsite geopolymer concrete (MCGC). In the first experimental group, via comparison with dry ceramsite (untreated), a method for modifying the ceramsite surface with a 6% silicone resin was proposed which could reduce its water absorption, enhance the compressive strength and slump of the corresponding concrete, and decrease the drying shrinkage. The second group systematically explored the influences of control factors on MCGC prepared from modified ceramsite. Different water/binder (w/b) ratios, [Na2O]/b ratios, and metakaolin content (MK/b) ratios were used in the experiment. Compressive strength and drying shrinkage tests were performed for 90 d. High w/b and Na2O/b ratios could enhance drying shrinkage. Moreover, 8% Na2O/b enhanced the compressive strength. Low compressive strength was obtained using 10% Na2O/b. A high MK/b ratio reduced drying shrinkage. However, high w/b and MK/b ratios hindered strength development. Finally, a model predicting drying shrinkage for MCGC with a high prediction accuracy was proposed by considering three control factors. Due to the variety of ceramsite pretreatment methods and the considered factor limitations, the model had potential for additional enhancements.
In this study, lightweight aggregate concrete [LWAC] was prepared by partially replacing cement with fly ash and partially substituting river sand with shell. The effects of fly ash and shell on the mechanical properties of concrete were studied by compressive test, splitting tensile test and flexural test. In addition, the specimens were microscopically analyzed by SEM electron microscopy. The results showed that both the compressive strength and splitting tensile strength decreased gradually with the increase of fly ash replacement ratio, but the maximum reduction was only 1.4 % and 3.1 % when the fly ash substitution ratio was 5 %. With the increase of shell replacement ratio, the compressive strength and splitting tensile strength of concrete increased first and then decreased, reached their maximum value at a substitution ratio of 10 %. The optimum fly ash substitution ratio and shell replacement ratio for LWAC were 5 % and 10 %, respectively. The compressive strength, splitting tensile strength and flexural strength of the experimental group under the optimum substitution ratio increased by 2.7 %, 0.6 % and 4.6 %, respectively, compared to the control group. The correlation coefficients of compressive strength with split tensile strength and flexural strength were 0.91 and 0.82, respectively. Finally, a compressive strength calculation formula related to fly ash substitution ratio and shell replacement ratio was proposed based on the Bolomy formula, and the correlation coefficient between the calculated value and the experimental value was 0.91.