The important role of natural organic matter (NOM)–Fe colloids in influencing contaminant transport, and this role can be influenced by the formation, aggregation, and particle deposition dynamics of NOM-Fe colloids. In this work, NOM-Fe colloids at different C/Fe ratios were prepared by mixing different concentrations of humic acid (HA) with 10 mg/L Fe(II) under anoxic conditions. The colloids were characterized by an array of techniques and their aggregation and deposition behaviors were examined under both anoxic and oxic conditions. The colloids are composed of HA-Fe(II) at anoxic conditions, while they are made up of HA-Fe(III) at oxic conditions until the C/Fe molar ratio exceeds 1.6. For C/Fe molar ratios above 1.6, the aggregation and deposition kinetics of HA-Fe(II) colloids under anoxic conditions are slower than those of HA-Fe(III) colloids under oxic conditions. Further, the aggregation of HA-Fe colloids under both anoxic and oxic conditions decreases with increasing C/Fe molar ratio from 1.6 to 23.3. This study highlights the importance of the redox transformation of Fe(II) to Fe(III) and the C/Fe ratio for the formation and stability of NOM-Fe colloids that occur in subsurface environments with anoxic–oxic interfaces.
Aqueous aggregation processes can significantly impact function, effective toxicity, environmental transport, and ultimate fate of advanced nanoscale materials, including graphene and graphene oxide (GO). In this work, we have synthesized flat graphene oxide (GO) and five physically crumpled GOs (CGO, with different degrees of thermal reduction, and thus oxygen functionality) using an aerosol method, and characterized the evolution of surface chemistry and morphology using a suite of spectroscopic (UV-vis, FTIR, XPS) and microscopic (AFM, SEM and TEM) techniques. For each of these materials, critical coagulation concentrations (CCC) were determined for NaCl, CaCl2, and MgCl2 electrolytes. The CCCs were correlated with material ζ-potentials (R2 = 0.94-0.99), which were observed to be mathematically consistent with classic DLVO theory. We further correlated CCC values with CGO chemical properties including C/O ratios, carboxyl group concentrations, and C-C fractions. For all cases, edge-based carboxyl functional groups are highly correlated to observed CCC values (R2 = 0.89-0.95). Observations support the deprotonation of carboxyl groups with low acid dissociation constants (pKa) as the main contributors to ζ-potentials and thus material aqueous stability. We also observe CCC values to significantly increase (by 18-80%) when GO is physically crumpled as CGO. Taken together, the findings from both physical and chemical analyses clearly indicate that both GO shape and surface functionality are critical to consider with regard to understanding fundamental material behavior in water.