An anti-oxidant Cu layer was achieved by remote mode N2 plasma. Remote mode plasma treatment offers the advantages of having no defect formation, such as pinholes, by energetic ions. In this study, an activated Cu surface by Ar plasma chemically reacted with N free radicals to evenly form Cu nitride passivation over the entire Cu surface. According to chemical state analysis using XPS, Cu oxidation was effectively prevented in air, and the thickness of the Cu nitride passivation was within 3 nm. Based on statistical analysis using the DOE technique with N2 plasma variables, namely, RF power, working pressure, and plasma treatment time, we experimentally demonstrated that a lower RF power is the most effective for forming uniform Cu nitride passivation because of a lower plasma density. When the N2 plasma density reached approximately 109 cm−3 in which the remote mode was generated, high energy electrons in the plasma were significantly reduced and the amount of oxygen detected on the Cu surface was minimized. Finally, low temperature (300 °C) Cu–Cu bonding was performed with a pair of the anti-oxidant Cu layers formed by the remote mode N2 plasma. Cu atomic diffusion with new grains was observed across the bonded interface indicating significantly improved bonding quality over bare Cu–Cu bonding.
Advanced packaging technology, also known as system scaling, bridges the gap between chip and package sizes by mounting multiple chips on a single package substrate. 2.5D packaging utilizing a passive device has been widely adopted and showed enhanced capacity and performance. However, 2.5D packaging presents its own challenges related to thermo-mechanical reliability because of large size of silicon interposer. This article reviews academic and industrial efforts to address the thermo-mechanical challenges associated with 2.5D packaging, particularly silicon interposer, focusing on the warpage and board-level interconnect reliability. The topics include simulation and measurement methods to evaluate and predict the thermo-mechanical characteristics of package components, such as warpage and strain distribution, as well as fatigue and lifetime of ball grid arrays. The impacts of materials and geometrical design factors are also discussed. Finally, challenges of current approaches and outlooks are presented.
12 July 2019 in IEEE Transactions on Components, Packaging and Manufacturing Technology
The success of wafer-to-wafer or chip-to-chip bonding in 3-D packaging relies on the development of planarized, activated, and oxygen-free Cu surface. Preventing Cu oxidation is becoming a crucial issue in chip-to-chip bonding processes. In this study, a two-step plasma pretreatment process was demonstrated to prevent copper oxidation by virtue of forming a nitride passivation layer on the Cu surface. The two-step plasma pretreatment consisted of Ar plasma to activate the Cu surface, followed by N2 plasma to passivate the Cu surface. It was found that the pressure in the Ar plasma step had the greatest effect on the formation of nitrate passivation on the Cu surface, and the lower the pressure in the Ar plasma step, the better the formation of copper nitrate in the N2 plasma step. The two-step plasma pretreatment provided a nitride-passivated Cu surface and significantly improved the Cu-to-Cu bonding quality. This process may enable Cu-to-Cu bonding in an atmospheric environment.
Low-temperature solderless Cu-Cu bonding is an important technology for advanced packaging, such as fine-pitch 3-D packaging and heterogeneous integration. In this study, we prepared an oxidation-free Cu surface using an optimized N 2 plasma process in a two-step Ar/N 2 plasma treatment based on the design of the experiment method, to improve direct Cu-Cu bonding quality at 260 °C. The N 2 plasma treatment process was optimized using the Minitab optimizer with chemical state results obtained by X-ray photoelectron spectroscopy (XPS) analysis. The Cu surface treated under the two-step Ar/N 2 plasma with optimized N 2 plasma conditions not only formed Cu nitride well, but the surface remained without further oxidation for at least one week at room temperature. The Cu-Cu bonding was performed at the low bonding temperature of 260 °C and low bonding pressure of 0.9 MPa for 1 hour, and the bonded interface was evaluated using scanning acoustic tomography (SAT) and field emission scanning electron microscope (FE-SEM) images. We measured shear strength to estimate the bonding interface quality of the oxidation-free Cu-Cu bonding specimen. A maximum shear strength of 62.6 MPa was obtained. Our bonding results demonstrated remarkably improved Cu-Cu bonding quality compared with other previous Cu-Cu joint studies that used Sn, Cu/Ag nanoparticles, or Cu composites.