10 March 2021 in IEEE Transactions on Components, Packaging and Manufacturing Technology
Low-temperature solderless Cu-Cu bonding is an important technology for advanced packaging, such as fine-pitch 3-D packaging and heterogeneous integration. In this study, we prepared an oxidation-free Cu surface using an optimized N 2 plasma process in a two-step Ar/N 2 plasma treatment based on the design of the experiment method, to improve direct Cu-Cu bonding quality at 260 °C. The N 2 plasma treatment process was optimized using the Minitab optimizer with chemical state results obtained by X-ray photoelectron spectroscopy (XPS) analysis. The Cu surface treated under the two-step Ar/N 2 plasma with optimized N 2 plasma conditions not only formed Cu nitride well, but the surface remained without further oxidation for at least one week at room temperature. The Cu-Cu bonding was performed at the low bonding temperature of 260 °C and low bonding pressure of 0.9 MPa for 1 hour, and the bonded interface was evaluated using scanning acoustic tomography (SAT) and field emission scanning electron microscope (FE-SEM) images. We measured shear strength to estimate the bonding interface quality of the oxidation-free Cu-Cu bonding specimen. A maximum shear strength of 62.6 MPa was obtained. Our bonding results demonstrated remarkably improved Cu-Cu bonding quality compared with other previous Cu-Cu joint studies that used Sn, Cu/Ag nanoparticles, or Cu composites.
19 May 2023 in IEEE Transactions on Components, Packaging and Manufacturing Technology
One of the key requirements for mass production of die-to-wafer Cu bonding is preventing copper surface oxidation. In this study, Cu bonding utilizing an Ag nanolayer was examined to achieve both Cu surface oxidation prevention and low-temperature bonding. The primary focus was to evaluate the impact of the annealing process on the Cu bonding quality. The Cu surface was coated with a 15 nm thick layer of Ag using evaporation technique. Cu wafer-to-wafer bonding was performed at a temperature of 180°C for 30 min, followed by annealing at 200°C for 60 min. The annealing process resulted in complete diffusion of Cu into the bonding interface, leading to a uniform and pure Cu-to-Cu bonding. However, the Ag nanolayer did not completely dissolve into the Cu thin film and formed a thin Ag band. The average shear strength of the specimens subjected to the annealing process was ~6.5 MPa., which was relatively low. Nonetheless, the annealing process has proven to be a very effective way to create a homogeneous bonding interface and achieve pure Cu-Cu bonding when using Ag nanolayers in Cu bonding.
1 January 1998 in MRS Proceedings