It is of great significance to develop carbon quantum dots (CQDs) using green carbon sources, which are cheap, non-toxic and harmless, and further expand their application scopes, e.g., fluorescence sensors, blue light screening. In this study, we have prepared Peperomia tetraphylla-based carbon quantum dots (PT-CQDs) with strong water solubility, good salt resistance, specific quenching reactions and excellent optical properties via a simple one-step hydrothermal method. In one application, PT-CQDs are utilized as a fluorescence sensor due to their high selectivity and sensitivity to ferric ions (Fe3+). The limit of detection (LOD) was 2.7 μmol·L−1. On the other hand, PT-CQDs/polyvinyl alcohol (PVA) films with excellent ultraviolet- (UV) and high-energy blue light (HEBL)-blocking properties were obtained. The obtained films exhibited a high blue light weight blocking rate of 100% in UV and 80% in HEBL. The concentrations of the composites could also be controlled to achieve the desired light-blocking rate. In addition, the composites were able to absorb blue light and convert it to other forms of light. These properties suggest their potential applications in the development of advanced blue light screening and fluorescence sensors.
An aggregation-caused quenching (ACQ)-active polymer (PF), an aggregation-induced emission (AIE)-active polymer (PFTPE) and an aggregation-enhanced emission (AEE)-active polymer (PTTPE) were synthesized by tetraphenylethane (TPE), fluorene and thiophene moieties. Polyurethane (PU) foams modified by PF, PFTPE and PTTPE, namely PU-PF, PU-PFTPE and PU-PTTPE, using ultrasonication-assisted method have been prepared. A comparative study of PU-PF, PU-PFTPE and PU-PTTPE for detection explosives had been performed, and significant fluorescence quenching was observed with the introduction of PA solutions. The as-prepared PU-PF, PU-PFTPE and PU-PTTPE sensors exhibited a superior sensitivity for PA solutions with different concentrations. Remarkably, PU-PF gave a quenching efficiency of 96.2%, higher than 93.5% for PU-PFTPE and 86.7% for PU-PTTPE at a PA concentration of 180 µg·mL−1 in methanol, which was attributed to the effective energy transfer from the fluorophore (PF) to the nitro explosive (PA). This suggested that some ACQ polymers, applied to detect explosives, could afford better performances than AIE or AEE polymers through modification of structures and selection of adequate carriers. At the same time, these chemical sensors can be recycled many times.
PU foams modified with an AIE-active polymer (PSiTPE) with a Si–O and TPE backbone using an ultrasonication-assisted method have been prepared. The as-prepared foams show a high sensitive to PA solution and DNT vapor. Moreover, it could be re-used several times. It is a novel promising probe for the detection of explosives.
Two novel fluorescent polymers PPOPAF and PPOCzF, with N+ P–O− resonance structures inserted into the fluorene-alt-carbazole based backbone, were developed as blue emitters and hosts for an orange-red phosphor to realize fluorescent–phosphorescent (F–P) hybrid white polymer light-emitting diodes (WPLEDs). The polymers exhibit proper HOMO/LUMO energy levels, good thermal stability and high triplet energy (ET) levels. Devices using PPOPAF and PPOCzF as single emissive layers show deep-blue emission with CIE coordinates of (0.16, 0.10) and (0.17, 0.10), respectively. Moreover, in hybrid white devices, doping with various concentrations of iridium(III) bis(4-phenylthieno[3,2-c]pyridinato-N,C2) acetylacetonate (PO-01) (0.1%, 0.2%, 0.5 wt%), the PPOCzF-based devices give a significant improvement than that of PPOPAF. While the doping concentration is 0.1 wt%, a nearly standard white emission (CIE: 0.35, 0.33) was achieved. The maximum CE, PE, EQE of PPOCzF-based devices is 4.4 cd A−1, 1.1 lm W−1, and 1.7%, respectively.
Long-chain hyperbranched polyesters (LHBPx, x = 1, 2, 3) with varying lengths of branched chains were synthesized through a thiol-ene click reaction. Subsequently, LHBPx was incorporated into PA4 via the solution method to prepare a LHBPx/PA4 polymer blend, aiming to address the limitations of PA4, such as its narrow thermal processing window (△T = Td5−Tm) and high brittleness. The results demonstrated that the addition of LHBPx enhanced the △T of PA4 from 1.6 °C to 14.5 °C (LHBP3/PA4), increasing the rheological properties of LHBPx/PA4 polymer blends, thereby improving its thermal processability. Compared with PA4, the elongation at the break of the LHBP3/PA4 polymer blend was increased by 20.4%, and the brittle fracture was changed into a ductile fracture. The crystallinity of PA4 was greatly decreased, from 54.41% to 37.42%, owing to the incorporation of LHBPx, whereas Tm of PA4 had almost no change. It was explained that LHBPx hindered the crystal growth stage, whereas it promoted the nucleation stage of PA4, resulting in no significant change in crystal type. Moreover, the longer the branched chain of LHBPx was, the more pronounced the improvement in the thermal processability and toughness of PA4 became. Above all, this work was meaningful for the potential application of PA4 in industrial plastics.
18 October 2016 in Journal of Applied Polymer Science