The mechanical properties of framework materials significantly influence stress distribution and the long-term success of implant-supported prostheses. Although titanium, cobalt-chromium, zirconia, and polyether ether ketone (PEEK) are widely used, their biomechanical performance under dynamic loading conditions remains insufficiently investigated. This study aimed to evaluate the biomechanical behavior of four framework materials with different Young's modulus using dynamic finite element stress analysis. A 3D edentulous maxillary model was extracted from a computer tomography (CT) database. Bone level implants with conical connection designs were placed in the anterior (canine) and posterior (first molar) areas. Anterior implants were parallel, yet posterior implants were inclined distally by 30 degrees. According to the framework material, four groups were formed: cobalt-chromium (Co-Cr), zirconia (Zr), titanium (Ti), and polyether ether ketone (PEEK). For each framework material, twelve separate models of analysis were created by applying force in three different orientations. Dynamic forces were employed to replicate the chewing process. Principal and von Mises stresses were measured and evaluated. The PEEK framework exhibited the highest maximum von Mises stress values (372.55 MPa) on the abutment and the highest maximum principle stress values (59.27 MPa) in the cortical bone. The Co-Cr framework had the lowest minimum principle stress (3.98 MPa) in the trabecular bone. The displacements of the Co-Cr, Zr, Ti, and PEEK frameworks were 0.15 mm, 0.15 mm, 0.17 mm, and 0.35 mm, respectively. Frameworks having a greater Young's modulus are less susceptible to deformation.
Background: Short-term sintering may offer advantages including saving time and energy but there is limited evidence on the effect that altering sintering time has on the accuracy of monolithic zirconia crowns. The purpose of this in vitro study was to investigate the effect of shortened sintering time on the marginal and internal fit of 3Y-TZP and 4Y-TZP monolithic crowns. Methods: Sixty monolithic zirconia crowns were fabricated for the maxillary first molar tooth on the prefabricated implant abutment. Groups were created according to the material composition: 3Y-TZP Generation 1, 3Y-TZP Generation 2 and 4Y-TZP. Two different sintering protocols were performed: same final sintering temperature (1500 °C) and various rates of heating (10 °C/min and 40 °C/min), cooling down speed (− 10 °C/min and − 40 °C/min), holding time (45 and 120 minutes), and total sintering time (approximately 2 and 7 hours, respectively). The marginal and internal fit of the crowns were determined using the silicone replica technique. Comparisons between groups were analyzed using two-way ANOVA. Pairwise multiple comparisons were performed using t-test (p < 0.05). Results: The mean marginal gap values of 4Y-TZP zirconia revealed statistically significant increase for the short-term sintering protocol (p < 0.0001), while no difference was observed between the sintering protocols for the mean marginal gap values of 3Y-TZP groups. Although all groups showed clinically acceptable gap values, altering the sintering time had an effect on marginal fit of the crowns manufactured from 4Y-TZP zirconia. Conclusions: Shortening the sintering time may lead to differences within clinically acceptable limits. The manufacturer’s recommendations according to material composition should be implemented with care.
This study aimed to evaluate the effects of surface treatments and resin cement on the adhesion of ceramic and ceramic-like materials to titanium. A total of 40 specimens (5 mm diameter) of each material (lithium disilicate glass ceramic (LDGC—IPS e.maxCAD), lithium silicate glass ceramic (LSGC—VITA Suprinity) and a polymer-infiltrated ceramic network (PICN—Vita Enamic)) were fabricated using CAD/CAM technologies. In total, 120 titanium (Ti) specimens were divided into 12 groups, and half of the titanium specimens were tribochemically coated using CoJet. The titanium and all-ceramic specimens were cemented using either Self-curing adhesive cement (SCAC—Panavia 21) or a Self-curing luting composite (SCLC—Multilink Hybrid Abutment). After 5000 cycles of thermal aging, the shear bond strength (SBS) test was conducted using a universal testing machine. The failure modes of the specimens were analyzed using stereomicroscopy, and additionally, the representative specimens were observed using Scanning Electron Microscopy. ANOVA was used for the statistical analysis (p < 0.05). The post-hoc Duncan test was used to determine significant differences between the groups. The mean SBS values (mean ± STD) ranged from 15 ± 2 MPa to 29 ± 6 MPa. Significantly higher SBS values were acquired when the titanium surface was tribochemically coated (p < 0.05). The SCLC showed higher SBS values compared to the SCAC. While the LDGC showed the highest SBS values, the PICN presented the lowest. The tribochemical coating on the cementation surfaces of the titanium increased the SBS values. The specimens cemented with the SCLC showed higher SBS values than those with the SCAC. Additionally, the SCLC cement revealed a more significant increase in SBS values when used with the LDGC. The material used for restoration has a high impact on SBS than those of the cement and surface conditioning.
11 April 2026 in The Journal of Prosthetic Dentistry
The purpose of this study was to evaluate the effect of different framework materials and thermal aging on the shear bond strength (SBS) of gingiva-colored composites used in fixed dental restorations. A total of 270 samples (10 × 10 × 2 mm3) were prepared using titanium, zirconia, and modified polyetheretherketone (modified PEEK). Three gingiva-colored composites (Gradia Gum, Anaxgum, Nexco) were applied after surface polishing and sandblasting. All specimens were stored in water at 37 °C for 24 h, then half of each group was subjected to thermal aging consisting of 10,000 cycles at temperatures between 5 and 55 °C. SBS testing was performed using a universal testing machine with a crosshead speed of 1 mm/min. Bonding failures were analyzed under a stereomicroscope, and one sample from each group was examined using a scanning electron microscope. SBS data were analyzed using three-way ANOVA with composite type, framework material, and thermal aging as factors, followed by pairwise comparisons (SPSS 23.0; p < 0.05). The highest SBS was recorded for the zirconia framework combined with Gradia Gum, specifically in the group without thermal aging (p < 0.05), while the lowest was observed for zirconia combined with Nexco after thermal aging (p < 0.05). Adhesive failures were predominant in the modified PEEK groups, whereas mixed failures occurred more frequently in titanium and zirconia groups. Both composite type and framework material significantly influenced SBS values, with thermal aging having a detrimental effect across all groups. This study demonstrates that both framework material and composite type affect bond strength, with specimens not subjected to thermal aging maintaining better adhesion. Thermal cycling reduced SBS in all groups, although the extent varied by material combination.