This study aimed to evaluate the effects of surface treatments and resin cement on the adhesion of ceramic and ceramic-like materials to titanium. A total of 40 specimens (5 mm diameter) of each material (lithium disilicate glass ceramic (LDGC—IPS e.maxCAD), lithium silicate glass ceramic (LSGC—VITA Suprinity) and a polymer-infiltrated ceramic network (PICN—Vita Enamic)) were fabricated using CAD/CAM technologies. In total, 120 titanium (Ti) specimens were divided into 12 groups, and half of the titanium specimens were tribochemically coated using CoJet. The titanium and all-ceramic specimens were cemented using either Self-curing adhesive cement (SCAC—Panavia 21) or a Self-curing luting composite (SCLC—Multilink Hybrid Abutment). After 5000 cycles of thermal aging, the shear bond strength (SBS) test was conducted using a universal testing machine. The failure modes of the specimens were analyzed using stereomicroscopy, and additionally, the representative specimens were observed using Scanning Electron Microscopy. ANOVA was used for the statistical analysis (p < 0.05). The post-hoc Duncan test was used to determine significant differences between the groups. The mean SBS values (mean ± STD) ranged from 15 ± 2 MPa to 29 ± 6 MPa. Significantly higher SBS values were acquired when the titanium surface was tribochemically coated (p < 0.05). The SCLC showed higher SBS values compared to the SCAC. While the LDGC showed the highest SBS values, the PICN presented the lowest. The tribochemical coating on the cementation surfaces of the titanium increased the SBS values. The specimens cemented with the SCLC showed higher SBS values than those with the SCAC. Additionally, the SCLC cement revealed a more significant increase in SBS values when used with the LDGC. The material used for restoration has a high impact on SBS than those of the cement and surface conditioning.
Although fiber-reinforced composites are commonly used in dental practice, whether fiber-reinforced crowns and fixed partial dentures can be used as definitive prostheses remains to be determined. This study used scanning electron microscopy to evaluate the load-bearing capacity of non-reinforced and fiber-reinforced composite (FRC) molar crowns prepared by computer-aided design/computer-aided manufacturing (CAD/CAM). The crowns were fabricated from three empirical FRC blocks, one empirical composite block, and one commercial ceramic block. The FRC resin was prepared by mixing BaO silicate particles, E-glass fiber, and dimethacrylate resin. Specimens were divided into five groups (n = 10), differing in the amounts of filler, resin, and fiber. Crowns were statically loaded until fracture. One-way analysis of variance and Tukey's post hoc multiple comparison tests were used for statistical analyses. The groups showed significant differences in load-bearing capacity; empirical bidirectional FRC resin blocks had the highest capacity, while commercial ceramic blocks had the lowest capacity. Molar crowns formed from FRC resin blocks had higher load-bearing capacity compared to non-reinforced composite resin and ceramic blocks. These results show that fiber reinforcement increased the load-bearing capacity of molar crowns.
The purpose of this study was to evaluate the effect of different framework materials and thermal aging on the shear bond strength (SBS) of gingiva-colored composites used in fixed dental restorations. A total of 270 samples (10 × 10 × 2 mm3) were prepared using titanium, zirconia, and modified polyetheretherketone (modified PEEK). Three gingiva-colored composites (Gradia Gum, Anaxgum, Nexco) were applied after surface polishing and sandblasting. All specimens were stored in water at 37 °C for 24 h, then half of each group was subjected to thermal aging consisting of 10,000 cycles at temperatures between 5 and 55 °C. SBS testing was performed using a universal testing machine with a crosshead speed of 1 mm/min. Bonding failures were analyzed under a stereomicroscope, and one sample from each group was examined using a scanning electron microscope. SBS data were analyzed using three-way ANOVA with composite type, framework material, and thermal aging as factors, followed by pairwise comparisons (SPSS 23.0; p < 0.05). The highest SBS was recorded for the zirconia framework combined with Gradia Gum, specifically in the group without thermal aging (p < 0.05), while the lowest was observed for zirconia combined with Nexco after thermal aging (p < 0.05). Adhesive failures were predominant in the modified PEEK groups, whereas mixed failures occurred more frequently in titanium and zirconia groups. Both composite type and framework material significantly influenced SBS values, with thermal aging having a detrimental effect across all groups. This study demonstrates that both framework material and composite type affect bond strength, with specimens not subjected to thermal aging maintaining better adhesion. Thermal cycling reduced SBS in all groups, although the extent varied by material combination.