3D printing of denture artificial teeth with resin materials is worthy of study in a novel way. This study evaluated chipping and indirect tensile fracture resistance of 3D printing resin material (Dentca 3D printing denture teeth resin) compared with conventionally prefabricated resin denture teeth (Premium-8, Surpass, SR-Orthosit-PE, and Preference). One hundred tooth specimens were prepared for testing. The 3D printed tooth specimens were printed at a 50 µm layer thickness with methacrylate-based photopolymerized resin by stereolithography 3D printing. Chipping and indirect tensile fracture tests were conducted at a speed of 1 mm/min until fracture. The indirect tensile fracture loads of the 3D printed resin teeth were higher than those of Premium-8, Surpass, and SR-Orthosit-PE, and lower than those of Preference teeth. Regarding chipping resistance, the 3D printed resin teeth were not different from Surpass and SR-Orthosit-PE, and were lower than Premium-8 and Preference teeth. The 3D printed resin teeth exhibited vertical fracture of the loaded cusp without deformation in chipping. The 3D printed resin teeth showed simultaneous fracture of two cusps in indirect tensile fracture, unlike other teeth. The results of this study suggest that 3D printing technology using resin materials provides adequate fracture resistance for denture artificial tooth use.
3D printing offers many advantages in dental prosthesis manufacturing. This study evaluated the wear resistance of 3D printing resin material compared with milling and conventional resin materials. Sixty substrate specimens were prepared with three types of resin materials: 3D printed resin, milled resin, and self-cured resin. The 3D printed specimens were printed at a build angle of 0° and 100 μm layer thickness by digital light processing 3D printing. Two kinds of abraders were made of zirconia and CoCr alloy. The specimens were loaded at 5 kg for 30,000 chewing cycles with vertical and horizontal movements under thermocycling condition. The 3D printed resin did not show significant difference in the maximal depth loss or the volume loss of wear compared to the milled and the self-cured resins. No significant difference was revealed depending on the abraders in the maximal depth loss or the volume loss of wear. In SEM views, the 3D printed resin showed cracks and separation of inter-layer bonds when opposing the metal abrader. The results suggest that the 3D printing using resin materials provides adequate wear resistance for dental use.
1 September 2020 in The Journal of Prosthetic Dentistry