Thermoplastic polyurethanes (TPUs) were synthetized with blends of poly(propylene glycol) (PPG) and poly(1,4-butylene adipate) (PAd) polyols, diphenylmethane-4,4′-diisocyanate (MDI) and 1,4-butanediol (BD) chain extender; different NCO/OH ratios were used. The structure and viscoelastic properties of the TPUs were assessed by infrared spectroscopy, differential scanning calorimetry, X-ray diffraction, thermal gravimetric analysis and plate-plate rheology, and their pressure sensitive adhesion properties were assessed by probe tack and 180° peel tests. The incompatibility of the PPG and PAd soft segments and the segregation of the hard and soft segments determined the phase separation and the viscoelastic properties of the TPUs. On the other hand, the increase of the NCO/OH ratio improved the miscibility of the PPG and PAd soft segments and decreased the extent of phase separation. The temperatures of the cool crystallization and melting were lower and their enthalpies were higher in the TPU made with NCO/OH ratio of 1.20. The moduli of the TPUs increased by increasing the NCO/OH ratio, and the tack was higher by decreasing the NCO/OH ratio. In general, a good agreement between the predicted and experimental tack and 180° peel strength values was obtained, and the TPUs synthesized with PPG+PAd soft segments had potential application as pressure sensitive adhesives (PSAs).
Wood plastic composites (WPCs) have poor adhesion properties due to their high surface concentration in non-polar polymers. In this work, two different plasma surface treatments, low pressure plasma (LPP) and atmospheric pressure plasma jet (APPJ), are proposed to increase the surface energy and adhesion property of WPC made with polyethylene (PE-WPC). After optimizing the conditions for each plasma surface treatment, the surface modifications and adhesion of PE-WPC treated with LPP and APPJ were compared. The optimal surface modifications of PE-WPC were obtained by treatment with Argon (Ar): Oxygen (O2) LPP for 90 s, and with air APPJ by using a plasma nozzle-WPC surface distance of one centimeter and speed of platform of one meter per minute. Both plasma treatments produced similar chemical modifications and surface energies on the PE-WPC surface. The ablation was more important for Ar:O2 LPP treatment, and the air APPJ treatment produced more extensive chemical modifications and more homogeneously removal of the wood component of the surface, rendering the polymer surface smoother. Adhesion of PE-WPC was similarly improved by treatment with both plasmas, from 56 N/m in the as-received to 92–102 N/m in the plasma treated PE-WPC joints. The influence of ageing at 24 °C and 40% relative humidity of the adhesive joints made with PE-WPC surface and treated with Ar:O2 LPP and APPJ plasmas was studied. In the joints made with plasma-treated PE-WPC aged under open air for more than one day, the adhesion decreased. An adhesive strength near to that of the joint made with the as-received PE-WPC was obtained after six days. However, if the adhesive joint was created immediately after plasma treatment and peeled at different times, the adhesion was maintained and even increased, and the hydrophobic recovery of the plasma-treated PE-WPC surface was inhibited.
Pressure sensitive adhesives made with blends of thermoplastic polyurethanes (TPUs PSAs) with satisfactory tack, cohesion, and adhesion have been developed. A simple procedure consisting of the physical blending of methyl ethyl ketone (MEK) solutions of two thermoplastic polyurethanes (TPUs) with very different properties—TPU1 and TPU2—was used, and two different blending procedures have been employed. The TPUs were characterized by infra-red spectroscopy in attenuated total reflectance mode (ATR-IR spectroscopy), differential scanning calorimetry, thermal gravimetric analysis, and plate-plate rheology (temperature and frequency sweeps). The TPUs PSAs were characterized by tack measurement, creep test, and the 180° peel test at 25 °C. The procedure for preparing the blends of the TPUs determined differently their viscoelastic properties, and the properties of the TPUs PSAs as well, the blending of separate MEK solutions of the two TPUs imparted higher tack and 180° peel strength than the blending of the two TPUs in MEK. TPU1 + TPU2 blends showed somewhat similar contributions of the free and hydrogen-bonded urethane groups and they had an almost similar degree of phase separation, irrespective of the composition of the blend. Two main thermal decompositions at 308–317 °C due to the urethane hard domains and another at 363–373 °C due to the soft domains could be distinguished in the TPU1 + TPU2 blends, the weight loss of the hard domains increased and the one of the soft domains decreased by increasing the amount of TPU2 in the blends. The storage moduli of the TPU1 + TPU2 blends were similar for temperatures lower than 20 °C and the moduli at the cross over of the moduli were lower than in the parent TPUs. The improved properties of the TPU1 + TPU2 blends derived from the creation of a higher number of hydrogen bonds upon removal of the MEK solvent, which lead to a lower degree of phase separation between the soft and the hard domains than in the parent TPUs. As a consequence, the properties of the TPU1 + TPU2 PSAs were improved because good tack, high 180° peel strength, and sufficient cohesion were obtained, particularly in 70 wt% TPU1 + 30 wt% TPU2 PSA.
About Me
Head and founder of the Adhesion and Adhesives Laboratory of the University of Alicante.
Head and founder of the Adhesion and Adhesives Laboratory of the University of Alicante.