In the present study, polycaprolactone/polyethylene glycol (PCL/PEG) electrospun nanofibres with different anthocyanin (1%, 2%, 3%, and 5%) were fabricated for the instant measurement of pH, especially for applications—such as food freshness detection—where quick response is required. The solution, surface, chemical, thermal, wettability, mechanical, and release properties of the samples were evaluated by viscosity measurements, scanning electron microscopy (SEM), Fourier‐transform infrared (FTIR), contact angle measurements, and tensile tests, respectively. The colorimetric analyses were also investigated against the solutions at different pH values and bacterial solutions. Finally, the on‐site performance of the sensor was evaluated. Anthocyanin addition initially lowered the solution viscosity, resulting in thinner fibres with a diameter of 288 nm. The diameters were increased up to 395 nm with the increasing anthocyanin. Anthocyanin addition enhanced the wettability and the mechanical properties, and the contact angles decreased to 43°. The highest modulus was observed for 1% anthocyanin, with a value of 6.162. The release experiments revealed that the anthocyanin‐loaded samples released a large amount of anthocyanin (between ~12% and 38%) in the first 15 s. The colorimetric analyses showed that PCL/PEG nanofibre mats with 2% and 3% anthocyanin concentrations were the most capable pH‐sensitive sensors for detecting pH changes from 2 to 8. As a result, it can be concluded that 3% anthocyanin is the threshold value for the production of the anthocyanin‐loaded nanofibre mats, and these structures are promising for the instant detection of pH proved by the on‐site application.
3 November 2010 in Journal of Applied Polymer Science
The effects of cross-sectional shape on the properties of cationic dyeable poly(ethylene terephthalate) fibres were investigated. Three different cross sections, namely tetra channel, snowflake and hollow, were used. Tensile test results showed that the hollow cross section has the highest breaking strength, while the snowflake has the lowest. In terms of thermal properties, no significant difference was observed. However, some differences in their morphology and surface topography were seen. According to birefringence studies, the hollow cross section has the highest overall orientation, while tetra has the lowest. In addition to this, hollow cross section gives the highest roughness value.
In the current study, a novel wound dressing material for an effective wound healing was developed by loading Uridine (URD), an endogenous compound known for its regenerative properties, into polycaprolactone (PCL) nanofibers. Initially, PCL nanofibers without URD were fabricated from different PCL solutions (7, 8, 10 and 11% w/w) by electrospinning and optimum PCL concentration (10% w/w) for URD loading was determined. After loading URD at different concentrations (0.1, 0.5 and 1% w/w) into 10% PCL solution, PCL/URD nanofibers were electrospun. Structural characteristics, release kinetics as well as in vitro and in vivo effects of the PCL/URD nanofibers were studied and in vivo effects were compared with a conventional wound dressing material. Loading URD increased nanofiber diameters from 248 to 509 nm and decreased contact angles from 123.76° to 94.3° with increasing URD concentrations. URD showed a burst release in the first 60 min following a more gradual release up to the 5th day which best fitted with Korsmeyer–Peppas model. PCL/URD mats provided enhanced viability in vitro in MTT assay using mouse L929 fibroblast cell line. Furthermore, in vivo wound closure studies revealed an immediate and robust wound healing in rats treated with PCL/URD mats compared to PCL mats without URD as well as the conventional wound dressing material. These data suggest that URD-loaded PCL nanofiber mats are promising materials as wound dressing. Graphical abstract