(1) Background: The failure of nickel–titanium (NiTi) rotary files is a complication related to endodontic instruments. The aim of this study was to compare the resistance to cyclic fatigue between rotary and reciprocating file systems. (2) Methods: Specific PICO: Population (P): artificial root canals; Interventions (I): instrumentation with NiTi rotary and reciprocating files; Comparison (C): rotary versus reciprocating files; Outcome (O): cyclic fatigue resistance. Studies were identified through bibliographic research using electronic databases (Medline, Embase, Scopus, SciELO, and WOS). The studies were combined using a random effects model by the inverse variance method. The effect size was the mean of the time to fracture (TTF) and number of cycles to fracture (NCF). Heterogeneity was assessed using the p value of the Q test for heterogeneity and the I2. (3) Results: TTF for rotary files was determined in 474.5 s and 839.1 for reciprocating without statistically significant differences. NCF for rotary systems was determined in 1444.2 and for reciprocating file systems in 4155.9 with statistically significant differences (p = 0.035), making reciprocating files more resistant. (4) Conclusions: Reciprocating files have better resistance to cyclic fatigue than rotary files. When tested in double curvature canals, reciprocating files also showed higher resistance.
Apical periodontitis is a common inflammatory condition associated with root canal treatment (RCT) failure. The quality of the three-dimensional root canal seal is critical to the success of the treatment. Bioceramic sealants, such as Neosealer Flo, offer biological advantages such as osteoconduction, biocompatibility and sustained calcium ion release, which may improve apical healing. The aim of this study was to compare AH Plus and Neosealer Flo in terms of postoperative pain, extrusion and periapical healing. A single-blind, randomised clinical trial was conducted with 60 patients divided into AH Plus and Neosealer Flo groups. Post-operative pain was assessed using a visual analogue scale (VAS) at 24 and 48 h and at 7 days. Seal quality and periapical healing were assessed at 6 months using the AAE success criteria by clinical and radiographic evaluation. Neosealer Flo resulted in less postoperative pain at 24 h and 7 days compared to AH Plus. Extrusion did not significantly affect pain or correlate with the type of sealer used. Both materials achieved similar periapical healing rates. Neosealer Flo demonstrated advantages in pain reduction, while both sealants showed comparable efficacy.
One of the most used rotary files in endodontics is NiTi files due to their superelastic properties. This property means that this instrument has extraordinary flexion that can adapt to large angles inside the tooth canals. However, these files lose their superelasticity and fracture during use. The aim of this work is to determine the cause of fracture of the endodontic rotary files. For this purpose, 30 NiTi F6 SkyTaper® files (Komet, Germany) were used. Their chemical composition was determined by X-ray microanalysis, and their microstructure was determined by optical microscopy. Successive drillings were carried out with artificial tooth molds at 30, 45, and 70°. These tests were carried out at a temperature of 37 °C with a constant load controlled by a high sensitivity dynamometer of 5.5 N, and every five cycles were lubricated with an aqueous solution of sodium hypochlorite. The cycles to fracture were determined, and the surfaces were observed by scanning electron microscopy. Transformation (austenite to martensite) and retransformation (martensite to austenite) temperatures and enthalpies were determined by Differential Scanning Calorimeter at different endodontic cycles. The results showed an original austenitic phase with a Ms temperature of 15 °C and Af of 7 °C. Both temperatures increase with endodontic cycling, indicating that martensite forms at higher temperatures, and the temperature must be increased with cycling to retransform it to austenite. This fact indicates the stabilization of martensite with cycling, which is confirmed by the decrease in both transformation and retransformation enthalpies. The martensite is stabilized in the structure due to defects and does not retransform. This stabilized martensite has no superelasticity and, therefore, fractures prematurely. It has been possible to observe the stabilized martensite by studying the fractography, observing that the mechanism is by fatigue. The results showed that the files fracture earlier the greater the angle applied (for the tests at 70° at 280 s, at 45° at 385 s, and at 30° at 1200 s). As the angle increases, there is an increase in mechanical stress, and, therefore, the martensite stabilizes at lower cycles. To destabilize the martensite, a heat treatment can be carried out at 500 °C for 20 min, and the files recovers all its superelasticity.
Aim: The aim of this study was to compare the cyclic fatigue strength of different reciprocating rotary systems depending on the movement used. Methods: Four study groups were analyzed (n = 30): (1) Reciproc®, (2) Reciproc Blue®, (3) Wave One Gold® and (4) Procodile®. Each group was divided into three subgroups according to the motion used: (A) Reflex Dynamic® (n = 10), (B) ReFlex Smart® (n = 10) and (C) conventional reciprocating motion (n = 10). They were used in a dynamic cyclic fatigue prototype until their fracture, and the time was measured in seconds. The results obtained were analyzed with the ANOVA method, and for two-to-two comparisons, the Tukey method and Weibull statistics were used. Results: Procodile ReFlex Smart had the longest time to failure, and statistically significant differences were found between Procodile ReFlex Smart and the other files and motions (p < 0.05). Conclusion: Smart motions increase cyclic fatigue strength. ReFlex Smart® motion increases the cyclic fatigue strength of reciprocating rotary systems, and Procodile® ReFlex Smart was the most resistant system file.
The aim of this paper was to assess the differences in tissue response to implantation during 15, 30 and 45 days in the subcutaneous connective tissue of Wistar rats from three biomaterials: Angelus MTA®, Theracal LC®, and Angelus MTA® to which 25% bioglass G3 was added. Twenty-four Wistar rats were used, the materials were inserted into the rat’s dorsal area in silicone tubes 5 mm long by 1.5 mm diameter. Histological reaction was assessed at 15, 30, and 45 days after implantation. They were then stained with hematoxylin eosin and evaluated by two observers. Data were analyzed using Fisher’s exact test and Mann–Whitney’s U test was used to determine the association between variables. Angelus MTA induced the formation of dystrophic calcifications twice as much as Theracal LC (p < 0.05). The addition of G3 did not affect the greater or lesser occurrence of calcifications (p > 0.05). Theracal LC and MTA plus G3 caused an inflammatory reaction, which was chronic at 15 days and decreased in intensity, almost disappearing after 45 days. Theracal LC, as well as Angelus MTA plus G3, were well tolerated when implanted in the subcutaneous connective tissue of rat. Histologically, no inconvenience was found for the use by direct contact of Theracal LC, and the mixture of MTA with 25% bioactive glass G3, in the tissue of Wistar rats.
The aim of this study was to evaluate ex vivo the sealing achieved at simulated lateral canals (SLC) and the quality of filling according to their position in the root canal after using the same filling technique. SLC were created at three levels in 55 teeth and divided into two groups depending on the root canal sealer used (1: BioRoot® RCS, 2: GuttaFlow® bioseal). They filled them with the continuous wave technique and submitted to a diaphanization technique. The samples were analyzed using a magnifying lens (20×), pictures were taken, which proceeded to linear measurement with the ImageJ® program and used a filling score system with five grades (0 to 4, 0 and 1 not acceptable, 2 to 4 acceptable); BioRoot® RCS has got a greater proportion than GuttaFlow® bioseal for SLC filled acceptably at 10 mm from the apex (p < 0.05). The highest proportion of SLC filled acceptably was found in the middle third (6 mm) (p < 0.05), followed by the apical third (3 mm) and the coronal third (10 mm). The difference between apical and coronal third could be significant; BioRoot® RCS has been better than GuttaFlow® bioseal for filling SLC in the coronal third of the teeth. Studies on the characteristics of these cements are missing to explain these differences.