Excellent mechanical properties and chemical stability make carbon nanotubes (CNTs) some of the most promising nanomaterials that can be used in cementitious composites to improve their performance. However, the difficulty of CNTs’ dispersion within the cementitious structure still exists and thus prevents the homogeneous distribution of CNTs. The homogeneous distribution of CNTs within a composite structure plays an essential role that can have a positive effect on the mechanical performance of CNT-cement composites. This paper introduces the methods for the production of CNTs and provides useful information about the influence of CNTs on the flowability, mechanical performance, microstructural changes and hydration of cement composites. The influences of water-cement ratio, used surfactants and various doses of CNTs on the properties of cementitious composites were also studied.
The synthesis of zeolite NaA from silica by-product was carried out in the presence of 20 kHz ultrasound at room temperature. Zeolites obtained in this type of synthesis were compared to zeolites obtained by performing conventional static syntheses under similar conditions. The sonication effects on zeolite NaA synthesis were characterized by phase identification, crystallinity etc. The effects of different parameters such as crystallization time and initial materials preparation methods on the crystallinity and morphology of the synthesized zeolites were investigated. The final products were characterized by XRD and FT-IR. It was possible to obtain crystalline zeolite NaA from by-product silica in the presence of ultrasound.
Concrete plants accumulate large amounts of concrete wash water. This water, which pH is highly alkaline, has a negative impact on the environment. Its reuse in fresh concrete slightly reduces its mechanical properties. The combination of concrete wash water and zeolitic by-product led to an increase of 4.6% in the compressive strength at 7 days hydration and up to 30% at 28 days hydration. The same combination led to the denser microstructure compared to the samples made with concrete wash water. This could be explained by the pozzolanic reaction of the zeolitic by-product. The complex chemical reactions of cement, zeolitic by-product, and fines presented in the concrete wash water occurred. Therefore, it was suggested the reusing method of concrete wash water together with zeolitic by-product in the fresh concrete mixtures by substituting some amount of tap water with concrete wash water. In this way, the consumption of tap water is possible to reduce in cement systems.
This paper deals with the behavior of concrete’s self-compatibility in a fresh state and its compressive and flexural strength in a hardened state with the addition of polyolefin macro fibers. Four different amounts (3 kg/m3, 4.5 kg/m3, 6 kg/m3, and 9 kg/m3) of polyolefin macro fibers were mixed into the concrete mixture to observe the differences in workability and strength properties between the concrete specimens. As a partial replacement of cement, class C type of fly ash was added to make up 25% of the total cement mass. The water-binder ratio (W/B) of the concrete mix was 0.36. Superplasticizer was added to the concrete mixture to achieve self-compacting properties. The slump test was carried out in the fresh state for determining the flowability. On the 7th and 28th days of the curing process, compression strength tests were performed, and on the 28th day, flexural strength tests and crack mouth opening displacement (CMOD) analyses were carried out to determine the strength properties and post-cracking behavior of the concrete samples. Bending strength and post-cracking behavior of the samples were improved by the addition of fibers. The fiber concentration in the concrete mixture greatly influenced the slump flow and self-compaction properties.