Qidong Zhang

Dr. Qidong Zhang


Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
20 February 2023 in Metals
Verified
Journal Article
Open access
PDF file
JSJianzhi Sun
Jianzhi Sun
HSHe Shang
He Shang
QZQidong Zhang
Qidong Zhang
XLXue Liu
Xue Liu
LCLiulu Cai
Liulu Cai
HYHan Yang
Han Yang
In this work, bio-hydrometallurgy technology was employed and a novel two-stage method based on successive chemical and bio treatments was proposed to collaboratively utilize manganese–silver ore and silver-bearing pyrite. In the optimization research of the chemical leaching stage, the sensitive factors for the Mn leaching efficiency were screened by Plackett–Burman design, and central compound design was performed to settle the optimized parameters. A mixed strain of bacteria containing Sulfobacillus thermosulfidooxidans, At. caldus and Leptospirillum ferrooxidans was applied in the bioleaching stage. A conventional cyanidation process carried out with the Mn leaching residuals suggested an efficient recovery of Ag. Applying a two-stage method with the optimum conditions, the leaching efficiency of 95.3% (Mn) and 96.3% (Ag) were obtained with 284.94 kg/t silver-bearing pyrite addition and 277.44 kg/t sulfuric acid consumption with a temperature at 77.73 °C and stirring speed at 287.76 rpm. Mineral behaviors were investigated with XRD and SEM/EDS analysis, and it was revealed that the oxidation of sulfur is the crux in reducing the usage of reagents, and the presence of leaching bacteria enhanced the oxidation efficiently. Through optimization and mechanism study, this paper provides an opportunity to co-leach the manganese–silver ore and silver-bearing pyrite process in a more economical and environmental way.

25 December 2021 in Metals
Verified
Journal Article
Open access
PDF file
Xinglan CuiXinglan Cui
Xinglan Cui
XYXuetao Yuan
Xuetao Yuan
HLHongxia Li
Hongxia Li
XCXiaokui Che
Xiaokui Che
JZJuan Zhong
Juan Zhong
QZQi Zheng
Qi Zheng
Exploring efficient methods to enhance leaching efficiency is critical for bioleaching technology to deal with sulfide concentrate. In our study, a novel artificial microbial community was established to augment the bioleaching efficiency and recovery of copper (Cu) and zinc (Zn). The optimum parameters in bioleaching experiments were explored according to compare a series of conditions from gradient experiments: the pH value was 1.2, temperature was 45 °C, and rotation speed was 160 r/min, which were different with pure microorganism growth conditions. Under optimal conditions, the result of recovery for Cu and Zn indicated that the average leaching rate reached to 80% and 100% respectively, which almost increased 1.8 times and 1.2 times more than control (aseptic condition) group. Therefore, this method of Cu and Zn recovery using a new-type artificial microbial community is expected to be an environmentally-friendly and efficient bioleaching technology solution, which has the potential of large-field engineering application in the future.

8 October 2026 in Materials
Verified
Journal Article
Open access
PDF file
ZHZhifang Hu
Zhifang Hu
BGBowen Gao
Bowen Gao
HJHonglin Jiang
Honglin Jiang
QZQidong Zhang
Qidong Zhang
YYYanxi Yin
Yanxi Yin
In this study, the iodide refining of high-purity vanadium metal was investigated experimentally and by two-dimensional numerical simulations based on the SIMPLE (Semi-Implicit Method for Pressure-Linked Equations) algorithm. The effects of system temperature, K values (characterizing the deposition filament temperature), initial iodine amount, and raw material packing configuration on the deposition rate, crystal morphology, and mass transport were studied in a custom-built iodide apparatus. The experimental results showed that the deposition rate exhibited a bell-shaped dependence on the source temperature. The optimal source temperature and optimal K value were 1123–1173 K and 40–50, respectively, at which the average deposition rate reached its peak. Both the average deposition rate and the average reaction time increased slightly with increasing initial iodine amount, but the increases were limited. Full loading of the raw material yielded crystal rods of uniform size. Vanadium crystal rods with a diameter of approximately 20 mm were obtained after refining. The metallic impurities Fe, Cr, Al, and Si were reduced to 0.025–0.033 wt.%, <0.001 wt.%, <0.001 wt.%, and <0.002 wt.%, respectively, while the interstitial impurities O, C, and N were reduced to <0.01 wt.%, <0.002 wt.%, and <0.002 wt.%, respectively, indicating that iodide refining can effectively reduce the contents of both interstitial and metallic impurities in vanadium metal. Numerical simulation results showed that the mass transport rate decreased monotonically with increasing total pressure, increased with rising temperature owing to the enhanced VI2 partial-pressure difference, and decreased with increasing transport distance. The flow pattern transitioned from pure diffusion/advection at 300 Pa to transitional vortices at 1000 Pa, and finally to fully developed recirculation at 3000 Pa. The simulation results are qualitatively consistent with the experimental observations, providing a theoretical basis for process optimization. To further improve the purity and scale-up potential of the process, it is necessary to conduct more in-depth research, including the development of fully coupled models that incorporate gas-phase dissociation, non-equilibrium surface kinetics, and composition-dependent mixture properties, as well as three-dimensional simulations and reactor material optimization.