This study focused on the development of Na+ ion sensing devices on a flexible substrate and investigated the impact of various additive materials on its sensing performance. For the Na+ ion sensing aspect, the film on the carbon working electrode used tert-butyl calix[4]arene tetraethyl acetate as the ion carrier. The main component of the film was polyvinyl chloride (PVC), with a plasticizer added to enhance its flexibility, ensuring better adaptation to the flexible substrate. In this base formulation, graphene oxide (GO) or multi-walled carbon nanotubes (MWCNTs) were incorporated into the sensing electrode to explore their effects on Na+ ion sensing capabilities. The results demonstrated that adding MWCNTs significantly improved the sensor’s sensitivity to Na+ ions. In addition, the study used the response slope to Na+ ions as a comparative reference for selectivity by calculating the ratio of the Na+ ion response slope to the response slopes of other ions (such as K+ and Ca2+). The findings showed that the sensors with MWCNTs exhibited better selectivity than the others with GO, and therefore, further analysis was performed on the response time of the sensors with MWCNTs. The results indicated that incorporating MWCNTs reduced the sensors’ response time and enhanced their overall sensitivity. However, excessive addition of MWCNTs would lead to a decrease in the selectivity of the fabricated sensors. This suggests that while MWCNTs offer promising improvements in performance, their concentration must be carefully optimized to maintain the sensors’ selectivity.
In this study, Mn2+ and Eu2+-codoped Sr3−xBaxMgSi2O8 (x = 0–1.5) phosphors were synthesized at 1400 °C under a reducing atmosphere composed of 5% H2 and 95% N2 to produce materials with blue light emission. The resulting powders were characterized using several analytical techniques: X-ray diffraction (XRD) was employed to identify the crystalline phases, scanning electron microscopy (SEM) was used to observe the microstructure, and photoluminescence excitation (PLE) and emission (PL) spectra were measured using a fluorescence spectrophotometer. The results revealed several key findings. XRD analysis showed that the Sr3MgSi2O8 (Sr3−xBaxMgSi2O8) phase coexisted with secondary phases of Sr2SiO4 and Sr2MgSi2O7. SEM observations indicated that the synthesized powders exhibited a distinctive needle-like structure anchored on the surfaces of the particles. The PL and PLE intensities increased sharply as the BaO content increased from x = 0 to x = 0.6, followed by a more gradual increase, reaching a peak at x = 1.2. Additionally, as the value of x increased, the wavelengths corresponding to maximum PL and PLE intensities exhibited a blue shift, moving to shorter wavelengths. Further investigation focused on the excitation behavior by replotting the PLE spectra using energy (eV) as the x-axis. A Gaussian fitting function was applied to deconvolute the excitation bands, enabling an in-depth analysis of how compositional variations influenced the Stokes shift.