In this study, Mn2+ and Eu2+-codoped Sr3−xBaxMgSi2O8 (x = 0–1.5) phosphors were synthesized at 1400 °C under a reducing atmosphere composed of 5% H2 and 95% N2 to produce materials with blue light emission. The resulting powders were characterized using several analytical techniques: X-ray diffraction (XRD) was employed to identify the crystalline phases, scanning electron microscopy (SEM) was used to observe the microstructure, and photoluminescence excitation (PLE) and emission (PL) spectra were measured using a fluorescence spectrophotometer. The results revealed several key findings. XRD analysis showed that the Sr3MgSi2O8 (Sr3−xBaxMgSi2O8) phase coexisted with secondary phases of Sr2SiO4 and Sr2MgSi2O7. SEM observations indicated that the synthesized powders exhibited a distinctive needle-like structure anchored on the surfaces of the particles. The PL and PLE intensities increased sharply as the BaO content increased from x = 0 to x = 0.6, followed by a more gradual increase, reaching a peak at x = 1.2. Additionally, as the value of x increased, the wavelengths corresponding to maximum PL and PLE intensities exhibited a blue shift, moving to shorter wavelengths. Further investigation focused on the excitation behavior by replotting the PLE spectra using energy (eV) as the x-axis. A Gaussian fitting function was applied to deconvolute the excitation bands, enabling an in-depth analysis of how compositional variations influenced the Stokes shift.
The synthesis process employed solid-state reaction methods to produce phosphors with varying CaO contents, specifically at x values of 0, 0.2, 0.4, 0.6, 0.8, and 1.0. As the CaO content (represented by the x value) increases, the crystalline structure of Ca2+xGa4O8+x + 0.01 Bi2O3 + 0.07 ZnO compositions underwent notable transformations. X-ray diffraction was used to characterize these structural changes, and we found that CaGa2O4, CaO, Ga2O3, and Ca3Ga4O9 were clearly identified. The diffraction intensities of CaGa2O4 and CaO phases increased and those of Ga2O3 and Ca3Ga4O9 decreased with the x value. Our findings revealed that the photoluminescence excitation (PLE) spectra consistently peak around 340 nm across all samples, while the photoluminescence emission (PL) spectra exhibited slight variations within the range of 474–477 nm. Most notably, the intensity of both PLE and PL spectra demonstrated a non-linear relationship with CaO content, initially increasing with higher CaO concentration, reaching maximum intensity at x = 0.4, and subsequently decreasing as the x value continued to rise. This research provides valuable insights into the relationship between composition, crystal structure, and luminescent behavior in Ca2+xGa4O8+x phosphor systems, and the theoretical mechanisms underlying these observed trends were thoroughly discussed.