Automated and robotic welding have become standard practices in manufacturing, requiring precise control to maintain weld quality without relying on skilled welders. In Tungsten Inert Gas (TIG) welding, monitoring the weld pool is crucial for ensuring the necessary weld penetration, which is vital for maintaining weld integrity. Real-time observation is essential to prevent defects and improve weld quality. Various sensing technologies have been developed to address this need, with vision-based systems showing particular effectiveness in enhancing welding quality and productivity within the framework of Industry 4.0. This review looks at the latest technologies for monitoring weld pools and bead shapes. It covers methods like using Complementary Metal-Oxide Semiconductors (CMOS) to take clear images of the melt pool for better process identification, Active Appearance Model (AAM) to capture 3D images of the weld pool for accurate penetration measurement, and Charge-Coupled Devices (CCD) and Laser-Induced Breakdown Spectroscopy (LIBS) to analyze plasma spectra and create material composition graphs.
25 July 2026 in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Laser powder-directed energy deposition enables near-net-shape fabrication of components using focused laser energy. In this study, a feedstock powder preheating technique was implemented to evaluate the mechanical and morphological characteristics. Initially, preheating temperatures of 55, 65, and 75 °C were applied for single-track investigation. Optimal performance was observed at 65 °C, resulting in improved geometry and a microhardness value of 204 HV (clad), indicating enhanced bonding and consolidation. A thin-wall structure fabricated using the optimized parameters was characterized in the bottom, middle, and top regions. The bottom region of the fabricated thin-wall structure exhibited peak ultimate tensile strength and yield strength of 664.99 and 461.47 MPa, respectively, which decreased by about 3% and 13% toward the top region, while elongation increased from 29.7% to 34.2%. The maximum Vickers hardness of 455.8 HV and Rockwell hardness of 45.08 HRC were observed in the top region. Optical microscopy identified epitaxial growth with columnar dendrites in the bottom zone, whereas the middle and top zones mainly exhibited columnar dendrites. Scanning electron microscopy fractography confirmed ductile fracture with dimple morphology, and energy-dispersive X-ray analysis provided microstructural insights. X-ray diffraction analysis confirmed a dominant γ-Fe austenitic phase, and atomic force microscopy revealed increased surface roughness from the bottom to the top region.