Processing, Microstructure and Properties of Laminated Ni-Intermetallic Composites Synthesised Using Ni Sheets and Al Foils: The laminated Ni-(NiAl3+Ni2Al3) and Ni-Ni2Al3intermetallic composites were fabricated by reaction synthesis in vacuum using Ni sheets and Al foils. The aluminium layers were completely consumed due to the formation of intermetallic phases. The Ni-Al reaction at 620°C was studied by interrupting in steps the reaction process to observe the microstructural changes. The final microstructure consisted of alternating layers of intermetallic phases and unreacted nickel can be designed easily because the stable structures of the composites depend only on the treating time. Microstructural examinations using scanning electron microscopy (SEM), X-ray diffraction (XRD) and X-ray microprobe analysis (EDX) demonstrated that after 1h of treatment Ni2Al3is the predominant intermetallic phase. The formation of the Ni2Al3phase is thermodynamically favoured over the formation of the other phases and can be understood from the steps occurred through a series of solid state reactions. The tensile strength of the laminated composites increases with an increase of the volume fraction of the intermetallic products. However, it decreases after long heat treatment because the Ni2Al3/Ni2Al3interfaces can very easily delaminate due to a very weak bonding caused by continuous Al2O3inclusions. Observations show that the laminated composites exhibit a mixture of brittle fracture of intermetallics and ductile one of residual Ni layers.
15 July 2007 in Materials Science and Engineering: A
Diffusion brazing was performed between titanium (Grade 2) and stainless steel (X5CrNi18-10) using as a filler a nickel foil at the temperatures of 850, 900, 950 and 1000°C. The microstructure was investigated using light microscopy and scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The stainless steel-nickel interface is free from any reaction layer at 850°C, above this temperature thin layer of reaction appears. The microhardness measured across the joints reaches higher values than for titanium and stainless steel, and it achieves value from 260 to 446 HV. The highest shear strength (214 MPa) was achieved for joints brazed at 900°C