This study investigates the influence of Y2O3 content and sintering temperature on the microstructure, phase composition, and physico-mechanical properties of zirconia-based ceramics with Al2O3 addition. It was shown that varying the stabilizer content within 3.0–6.0 wt.% Y2O3 leads to observable changes in the phase composition and grain size, as well as affecting the density and microhardness of the material. The sintering conditions ensuring the required density and homogeneous microstructure at moderate temperatures were determined. This research is aimed at optimizing synthesis and heat treatment parameters to produce a dense material with minimal porosity and stable mechanical characteristics. The samples were shaped by uniaxial pressing and sintered in the temperature range of 1530–1570 °C. The structure and phase composition were analyzed using X-ray diffraction and scanning electron microscopy, while the physico-mechanical properties were evaluated by measuring apparent density, porosity, and microhardness. The sintering temperature of 1550 °C was identified as optimal for achieving the highest performance characteristics while maintaining structural homogeneity. The addition of Al2O3 contributes to a reduction in the sintering temperature without compromising the material’s properties.
The effect of the partial substitution of Cu for Al on the structural, compositional, and magnetic properties of polycrystalline compounds YBa2Cu3O7−δ was studied. All prepared samples turned out to be single-phase with a small fraction of Ba secondary phases. Substitution of more than 2% aluminum causes an increase in spurious phases. DC susceptibility measurements show that the superconducting transition temperature T C decreases. Hysteresis loops show that magnetic irreversibility decreases with increasing Al content. The critical current density J C obtained using the Bean formula does not follow the same change. Al compensates for a decrease in J C and an increase in its content near the solubility limit gives a higher J C than in an undissolved sample.