19 July 2025 in Materials
Verified
Journal Article
Open access
PDF file
GWGang Wang
Gang Wang
RZRunbo Zhang
Runbo Zhang
XXXiangyu Xu
Xiangyu Xu
RYRen Yuan
Ren Yuan
LXLv Xvteng
Lv Xvteng
CFChenglei Fan
Chenglei Fan
This study develops an optimized femtosecond laser welding process for joining quartz glass and TC4 titanium alloy (Ti-6Al-4V) under non-optical contact conditions, specifically addressing the manufacturing needs of specialized photoelectric effect research containers. The joint primarily consists of parallel laser-welded zones (WZ) interspersed with base material. The defocus distance of the femtosecond laser predominantly influences the depth and phase composition of the WZ, while the weld spacing influences the crack distribution in the joint region. The maximum shear strength of 14.4 MPa was achieved at a defocusing distance of +0.1 mm (below the interface) and a weld spacing of 40 μm. The XRD stress measurements indicate that the defocusing distance mainly affects the stress along the direction of laser impact (DLI), whereas the weld spacing primarily influences the stress along the direction of spacing (DS). GPA results demonstrate that when the spacing is less than 30 μm, the non-uniform shrinkage inside the WZ induces tensile stress in the joint, leading to significant fluctuations in DS residual stress and consequently affecting the joint’s shear strength. This study investigates the effects of process parameters on the mechanical properties of dissimilar joints and, for the first time, analyzes the relationship between joint residual strain and femtosecond laser weld spacing, providing valuable insights for optimizing femtosecond laser welding processes.

11 October 2025 in Metals
Verified
Journal Article
Open access
PDF file
GWGang Wang
Gang Wang
XXXiangyu Xu
Xiangyu Xu
RZRunbo Zhang
Runbo Zhang
RYRen Yuan
Ren Yuan
LXLv Xvteng
Lv Xvteng
A Y-doped AlCoCrFeNi2.1 eutectic high-entropy alloy was fabricated via powder bed fusion-laser melting/metal (PBF-LB/M), and the effects of the rare-earth element Y on its microstructure and mechanical properties were investigated. The results indicate that Y addition preserves the fine eutectic microstructure inherent to the PBF-LB/M process, while inducing lattice distortion within the face-centered cubic (FCC) matrix and promoting grain refinement. During solidification, Y facilitates heterogeneous nucleation and, due to its strong affinity with Al, increases both the volume fraction of the body-centered cubic (BCC) phase and the proportion of high-angle grain boundaries. X-ray diffraction (XRD) analysis further confirms that Y suppresses the formation of the ordered B2 phase. Tensile testing reveals that Y doping improves the tensile strength from 1383 MPa to 1475 MPa and enhances the elongation from 13.0% to 16.3%. Fractography shows a transition from quasi-cleavage to ductile fracture mode, indicating that Y significantly enhances the strength–ductility synergy of the alloy.