The crystallization of polyethylene (PE) blends is a highly complex process, owing to the significant differences in crystallizability of the various PE components and the varying PE sequence distributions resulting from short- or long-chain branching. In this study, we examined both the resins and their blends through crystallization analysis fractionation (CRYSTAF) to understand the PE sequence distribution and differential scanning calorimetry (DSC) to investigate the non-isothermal crystallization behavior of the bulk materials. Small-angle X-ray scattering (SAXS) was utilized to study the crystal packing structure. The results showed that the PE molecules in the blends crystallize at different rates during cooling, resulting in a complicated crystallization behavior characterized by nucleation, co-crystallization, and fractionation. We compared these behaviors to those of reference immiscible blends and found that the extent of the differences is related to the disparity in crystallizability between components. Furthermore, the lamellar packing of the blends is closely associated with their crystallization behaviors, and the crystalline structure varies significantly depending on the components’ compositions. Specifically, the lamellar packing of the HDPE/LLDPE and HDPE/LDPE blends is similar to that of the HDPE component owing to its strong crystallizability, while the lamellar packing of the LLDPE/LDPE blend is approximately an average of the two neat components.
The effect of annealing on the microstructure and tensile properties of low-density polyethylene (LDPE) non-woven fabric produced by melt electrospinning was systematically investigated using DSC, SAXS, SEM, etc. The results showed that, above an annealing temperature of 80 , both the main melting point and crystallinity of LDPE decreased compared to the original sample, as did the tensile strength of the non-woven fabric. Additionally, the lamellar distribution became broader at annealing temperatures above 80 . The recrystallization mechanism of molten lamellae (disordered chains) in LDPE was elucidated by fitting the data using a Gaussian function. It was found that secondary crystallization, forming thicker lamellae, and spontaneous crystallization, forming thinner lamellae, occurred simultaneously at rates dependent on the annealing temperature. Secondary crystallization dominated at temperatures ≤80 , whereas spontaneous crystallization prevailed at temperatures above 80 . These findings explain the observed changes in the microstructure and tensile properties of the LDPE non-woven fabric. Furthermore, a physical model describing the microstructural evolution of the LDPE non-woven fabric during annealing was proposed based on the experimental evidence.
Polymers of higher olefin, obtained by Ziegler-type polymerization, have been used in some critical fields, e.g., as the membrane for extracorporeal membrane oxygenation (ECMO), which plays an important role in the treatment of patients with severe COVID-19. The polymer obtained by a single-site catalyst, e.g., metallocene catalysts, demonstrated a higher performance. The homo- and co-polymerization of allyltrimethylisilane (ATMS) and 4-methyl-1-pentene (4M1P) were conducted using syndiospecific (cat 1) and isospecific (cat 2) metallocene catalysts. Cat 1 showed low conversions and provided a polymer with a higher molecular weight, while cat 2 behaved oppositely. 13C-NMR spectra certified the stereotacticity of the resultant polymer, and the resonance of the carbon atom of CH2 (αα’) between the two tertiary carbon atoms of the ATMS and 4M1P units were observed. This could be the evidence of the formation of a true copolymer. The crystallization of the polymer was explored using a differential scanning calorimeter (DSC) and wide angle X-ray diffraction (WAXD). All homopolymers and some of the copolymers showed high melting temperatures and low melting enthalpies. The WAXD patterns of the syndiotactic polymer and isotactic homopolymer or the ATMS-rich copolymer were consistent with the reported literature, but the isotactic 4M1P-rich copolymer provided the crystal form I, which is unusual for a 4M1P polymer without any pretreatment.
Our experiment revealed that the addition of Janus nanosheets to polypropylene (PP) has a significant impact on the viscoelasticity of the composite system. Specifically, when 0.10 wt% of Janus nanosheets were added, the complex viscosity of the composite system increased. However, when we added less than 0.05 wt% of Janus nanosheets, there was a reduction in complex viscosity, which is known as the non-Einstein phenomenon. The Cole–Cole plot showed that the nanosheet network structure did not have a significant effect on the viscosity of the composite system. Additionally, we used carbon dioxide as a foaming agent to autoclave foaming using modified PP from Janus nanosheets, and the results demonstrated that increasing the number of Janus nanosheets decreased the apparent density and strengthened the cell structure of foaming beads, resulting in improved closed porosity.
Herein, we study comparatively the crystal structure, orientation, and residual stress of polypropylene (PP) films processed by uniaxial constant width (UCW) and uniaxial free width (UFW) stretching modes, respectively. Compared with UFW PP film, UCW PP film exhibits broad lamellar thickness distribution with thinner average lamellar thickness, and accordingly lower melting temperature region. UCW PP film also has larger lateral lamellar size with high orientation along stretching direction. In addition, a preferential orientation of b -axis perpendicular to the surface exists in the UCW PP film, while a cylindrical symmetry around the stretching direction is in UFW PP film. A new single tilt X-ray diffraction method is utilized to measure the residual stress of PP films. The direction of maximum principal tensile residual stress is approximately along stretching direction for both films, while tensile residual stress occurs in UCW PP film and compressive residual stress in UFW PP film in transverse direction. Good correlation of the direction of maximum residual stress with crystal orientation is found in both PP films.