This study explored the use of physical methods, namely X-ray diffraction, atomic force microscopy, and energy-dispersive X-ray spectroscopy, to analyze the structure and composition of tear fluid desiccates. Tear samples were collected from patients with dry eye syndrome, glaucoma, and multiple sclerosis. Our results revealed significant differences in the crystallization patterns, chemical composition, and morphology of tear fluid among the disease groups compared to healthy individuals. XRD analysis identified variations in salt crystallization within tear fluid desiccates. AFM provided nanoscale morphological visualization. EDX determined the presence of key chemical elements. Our findings showed that changes in crystallization and unbalance of ionic composition in tear fluid may serve as potential markers for diagnosing ocular diseases. This study highlights the potential of these techniques for non-invasive diagnostics and contributes to the development of innovative strategies for monitoring structural properties in tear fluid desiccates of analyzed inflammatory, and neurodegenerative diseases.
Non-equiatomic high-entropy alloys (HEAs) are promising candidates for low-dimensional magnetocaloric applications. In this work, Fe25Ni21Mn24Si13Ge17 HEA-based nanoribbon arrays with spacings of 1 and 2 µm, together with companion thin films, were fabricated under the same technological conditions by magnetron co-sputtering from five sources. The effects of heat treatment and longitudinal strain (0–2%) on the structural, magnetic, and magnetocaloric properties were studied using TEM, SAED, AFM, and SQUID magnetometry. TEM, SAED, and AFM confirmed an amorphous structure with a single cubic-type short-range order and thermal stability up to 700 K. The nanoribbons exhibited shape-induced magnetic anisotropy that vanished at a 2 µm spacing, where the ribbons became magnetically decoupled. Within the elastic regime, longitudinal strain acted via magnetoelastic coupling, preserving the in-plane isotropy while enhancing the magnetic response above 100 K. Annealing at 700 K drove short-range atomic reordering and relieved fabrication-induced strain, increasing the saturation magnetization severalfold and raising the maximum isothermal magnetic entropy change −ΔSM of the 1 µm nanoribbons from 1.25 to 1.35 JK−1kg−1 (at 140 K, ΔH = 50 kOe). The results demonstrate that strain engineering and thermal processing provide distinct, complementary routes for tuning the magnetic and magnetocaloric behavior of FeNiMnSiGe HEA nanoribbons.
The influence of the effective Dy layer thickness and temperature of the heat treatment on the structural-phase state, electrophysical and magnetoresistive properties of three-layer Ni/Dy/Co films have been analyzed. The research result of the phase composition investigation in the as-deposited state corresponds to fcc-Ni + hcp-Co + fcc-Co + qa-Dy. It was determined that the system is characterized by a relatively large value of the temperature coefficient of resistance (~10 -3 K -1 ) and has resistivity of the order of ρ~ 10 -6 Om m, that is due to the presence of a large number of defects in the crystalline system structure. The investigation in the as-deposited state indicates an anisotropic behavior of the magnetoresistance dependence, the magnitude of which varies with the change in the effective thickness of the Dy layer. The heat treatment within the limits of 500-800 K does not lead to a change in the phase composition and the nature of the dependence of magnetoresistance (B), but only causes recrystallization processes and changes in the value of the magnetoresistance amplitude. The sharp change in the magnetoresistance and the coercive force with the change of the orientation of the sample in the external magnetic field allows to consider these films as a sensitive element of the AMR-sensor.