In Directed Energy Deposition (DED), modeling the molten pool temperature field is crucial for precise temperature control, process optimization, and quality improvement. However, conventional numerical methods suffer from limitations such as high computational costs and poor transferability. This study proposes a physics-informed neural network with dynamic learning rate (DLR-PINN) model, which integrates transfer learning to enable rapid prediction of 3D temperature fields and dimensions of molten pools across process parameters. Its validity is verified by a finite element method (FEM) calibrated via single-track DED experiments. Results show that DLR-PINN exhibits superior convergence and stability compared to traditional PINN. Combined with transfer learning, training efficiency is significantly enhanced, with a single prediction taking only 10 s. Using the FEM as the benchmark, it achieves a mean absolute percentage error (MAPE) of 0.53% for temperature prediction, and MAPE of 3.69%, 2.48%, and 6.96% for molten pool dimension predictions, respectively. Sensitivity analysis of process parameters reveals that scanning speed has a significantly greater regulatory effect on molten pool characteristics than laser power. Additionally, the temperature field of the flat-top heat source is more uniform than that of the Gaussian heat source, which is more conducive to improving printing quality and efficiency.
This paper investigates WC-10Co4Cr coatings on 4340 steel prepared by conventional HVOF and novel cold spraying (CS) under optimal process parameters to address low wear resistance. The results show that the CS WC-10Co4Cr coating porosity is less than 0.1%, while the HVOF WC-10Co4Cr coating porosity is about 0.3%. The WC phase in the CS coating did not change, whereas the WC phase in the HVOF coating underwent decarburization and a new W2C phase was formed. The microhardness of the CS WC-10Co4Cr coating reaches 1617.2 HV0.3, which is about 50% higher than that of HVOF WC-10Co4Cr coating of 1061.3 HV0.3. The sliding wear rate of the CS WC-10Co4Cr coatings is 0.17 × 10−5 μm3/N·m, which is 40% of that of the HVOF coatings. The CS coating’s fretting wear rate is 1.28 μm3/N·m, which is 40% faster than that of HVOF coating. However, the bond strength of the CS WC-10Co4Cr coating (35 MPa) is lower than that of the HVOF coating (73.5 MPa). Overall, the WC-10Co4Cr coatings prepared by the CS process have higher hardness, denser coating microstructure, and better sliding wear resistance than those prepared by the conventional HVOF process.