This research evaluates the mechanical properties of a variety of binary In-Sn alloys as potential candidates for low temperature electronic joints. The tensile and hardness tests of as-cast In-5Sn, In-12.5Sn, In-25Sn, In-30Sn, In-35Sn, In-40Sn, In-50Sn, In-60Sn, In-80Sn (wt.%) were assessed at room temperature and compared to those of pure In and Sn. The ultimate tensile strength (UTS) increased from 4.2 MPa to 37.8 MPa with increasing tin content in the alloys under the testing condition of 18 mm/min and the results showed little difference under a lower strain rate (1.8 mm/min). Most compositions showed good ductility in tensile testing with an average of 40% elongation. A melting point range of 119.3 °C to 194.9 °C for tested alloys was measured using differential scanning calorimetry (DSC). The microstructure investigated by scanning electron microscopy (SEM) was discussed with respect to the mechanical properties and it has been found that the presence of the Sn-rich γ-InSn4 phase in the microstructure has a significant impact on mechanical properties. The fundamental data from this study can be used for the development of new low temperature In-Sn alloys.

25 July 2024 in Materials
Verified
Journal Article
Open access
PDF file
JZJiye Zhou
Jiye Zhou
Xin Fu TanXin Fu Tan
Xin Fu Tan
SMStuart M. Mcdonald
Stuart M. Mcdonald
Kazuhiro NogitaKazuhiro Nogita
Kazuhiro Nogita
The In–Bi–Sn low-temperature solder alloys are regarded as potential candidates for cryogenic and space exploration applications. This study investigates the variations in the mechanical properties and microstructures of two different compositions: In15wt%Bi35wt%Sn and In30wt%Bi20wt%Sn, after exposure to a low-temperature environment (−20 °C) for 10 months. An increase in the ultimate tensile strength was observed across all the tested samples and a decrease in elongation to failure was observed in In30wt%Bi20wt%Sn. Changes in the microstructure were identified through scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD). The impact of this low-temperature environment is described, considering the varying proportions and compositions of the three phases (BiIn2(Sn), γ-InSn4(Bi), and β-In3Sn(Bi)) present within the alloys and their contribution to the mechanical properties.

31 July 2025 in Materials Science and Engineering: A
Verified
Journal Article
Open access
JZJiye Zhou
Jiye Zhou
Xin Fu TanXin Fu Tan
Xin Fu Tan
QGQinfen Gu
Qinfen Gu
SMStuart D. McDonald
Stuart D. McDonald
Kazuhiro NogitaKazuhiro Nogita
Kazuhiro Nogita

21 August 2025 in Materials
Verified
Journal Article
Open access
PDF file
Kazuhiro NogitaKazuhiro Nogita
Kazuhiro Nogita
Xin Fu TanXin Fu Tan
Xin Fu Tan
JZJiye Zhou
Jiye Zhou
SMStuart M. Mcdonald
Stuart M. Mcdonald
KSKeith William Sweatman
Keith William Sweatman
Christopher M. GourlayChristopher M. Gourlay
Christopher M. Gourlay
For reliable electronics, it is important to have an understanding of solder joint failure mechanisms. However, because of difficulties in real-time atomistic scale analysis during deformation, we still do not fully understand these mechanisms. Here, we report on the development of an innovative in situ method of observing the response of the microstructure to tensile strain at room temperature using high-voltage transmission electron microscopy (HV-TEM). This technique was used to observe events including dislocation formation and movement, grain boundary formation and separation, and crack initiation and propagation in a Sn-3 wt.%Ag-0.5 wt.%Cu (SAC305) alloy joint formed between copper substrates.

8 July 2025 in Preprints.org
Verified
Preprint
Open access
PDF file
Kazuhiro NogitaKazuhiro Nogita
Kazuhiro Nogita
Xin Fu TanXin Fu Tan
Xin Fu Tan
JZJiye Zhou
Jiye Zhou
SMStuart M. Mcdonald
Stuart M. Mcdonald
KSKeith William Sweatman
Keith William Sweatman
Christopher M. GourlayChristopher M. Gourlay
Christopher M. Gourlay
If electronics manufacturers and users are to have confidence in the reliability of the solder joints on which they rely, it is essential to have an understanding of the solder joint failure mechanisms and the role of dynamic recrystallisation in failure. However, due to difficulties in real-time atomistic scale analysis during deformation, we still do not fully understand these mechanisms. Here, we report the development of an innovative in-situ method using high voltage transmission electron microscopy (HV-TEM) for observation of the microstructural response of a solder joint to room temperature tensile loading. This technique was used to observe events including dislocation formation, dynamic recrystallisation, grain boundary separation, and crack formation and propagation in a Sn-3wt.%Ag-0.5wt.%Cu (SAC305) alloy joint formed between copper substrates.