This research presents an experimental investigation on the compressive behavior of fiber reinforced polymer-confined concrete-filled steel tubes (FRP-CFSTs). The study evaluated 72 specimens, including CFST and FRP-CFST columns, with varying numbers of FRP layer (0–3), steel tube thickness (1.8 to 3.8 mm), and nominal concrete strength (20, 30, 40 MPa). Concrete mixes enhanced with polypropylene fibers and silica fume were used. Material properties for the infill concrete, steel tube yield strength (307 MPa), and CFRP tensile parameters (ultimate strain 2.1%, tensile strength 4900 MPa) were determined. The test specimens were wrapped with CFRP sheets using a wet lay-up process and subjected to axial compression through a 4000-kN capacity machine. The load–deformation behavior until failure, which typically occurred due to FRP rupture from lateral concrete expansion, was recorded. Results revealed that FRP confinement increased the ultimate axial load capacity of CFST columns and enhanced ductility with improvements correlating positively with the number of CFRP layers. Steel tube thickness contributed to an increase in stiffness and load capacity by roughly 15–25%. Concrete mixes incorporating polypropylene fibers and silica fume demonstrated superior performance compared to conventional mixes by reducing brittleness and improving tensile and flexural strengths. These quantitative findings demonstrate the significant influence of FRP confinement and concrete mix design on the enhancing strength, stiffness, and ductility of CFST columns, supported by rigorous experimental characterization and systematic analysis of their composite behavior.
This paper portrays an experimental study to understand the compressive performance of FRP-confined concrete-filled steel tube (FCCFST). Columns CFST columns have large strength and good deformability characteristics which make it precious structural members. The large lateral stiffness and strength, as well as the large load-carrying capacity that is obtained by a steel tube and concrete interaction, are sufficiently procured in the CFST columns. Concrete-filled steel tube columns are promoted for superior performance due to the composite action between the concrete core and the steel tube. However, the full potential of this composite action is often not realized because of the differing dilation properties between the materials, which could lead to debonding at the interface. To address this issue, external confinement using FRP is proposed to enhance the bonding between the concrete and steel tube. In this study, seventy-two columns were verified to examine the effects of various factors, including the number of carbon fiber reinforced polymer (CFRP) layers, steel tube thickness, and infilled concrete properties (with and without silica slurry and polypropylene fiber) on the columns' load capacity and axial deformation capacity. The experimental load-carrying capacity of the columns was also compared with those obtained from existing formulations proposed by some researchers. It is observed that the external CFRP wrap helps constrain the steel tube's outward local buckling deformation and enhances the concrete core's confinement. The results also demonstrate that CFRP confinement significantly improves the load capacity and axial distortion capacity of the CFST columns. The prediction performance of existing formulations was varied, however, one of the proposed ones estimates the experimental values with reasonable accuracy.
30 August 2023 in Asian Journal of Civil Engineering
This study develops and experimentally verifies nonlinear finite element models for carbon-fiber-reinforced (CFRP) confined concrete-filled steel tube (CFST) columns under axial compression. ABAQUS- based 3D models represent the steel tube, concrete core and CFRP wrap using C3D8R solid elements and S4R shell elements, respectively, with contact interactions to capture interface behavior. Concrete is modeled with the concrete damage velocity (CDP) model steel and (CFRP) adopt bilinear and orthotropic elastic – plastic/elastic constitutive laws. Validation uses an experimental database of 72 columns (18 CFST,54 CFRP- confined) varying steel thickness (1.8-3.8mm) concrete strength (20-40 MPa), and CFRP layers (0-3). Numerical load- shortening curves, ultimate loads and failure modes closely match tests (Nu, exp/Nu,FEM=0.83-1.08) parametric studies show that increasing CFRP layers raises peak load and ductility and smooths post-peak softening, but concrete strength and steel thickness exert equal or greater influence on axial capacity. Modeled stress field reveal that CFRP delay outward steel deformation, promotes uniform stress distribution and mitigates local buckling. The validated models quantify confinements effects and provide insight in to interaction mechanics among concrete, steel, and CFRP. Results support the use of the FE framework for design-oriented parametric studies and for developing practical predication tools for CFRP- strengthened CFST columns.
This study develops and evaluates a three-dimensional nonlinear finite element (FE) framework for carbon fiber-reinforced polymer (CFRP)-confined concrete-filled steel tube (CFST) short columns subjected to concentric axial compression. The concrete core is represented using C3D8R solid elements, and the steel tube and CFRP jacket using S4R shell elements. Concrete is modeled with the concrete damage plasticity (CDP) formulation, the steel tube with an elastic–plastic constitutive law, and the CFRP jacket with an orthotropic elastic law. The FE framework is evaluated against the 72-column experimental database reported previously comprising 18 unwrapped CFST specimens and 54 CFRP-confined specimens. The database covers steel tube thicknesses of 1.8–3.8 mm, measured concrete strengths of 19.3–39.8 MPa, and 0–3 CFRP layers. No constitutive parameter was fitted to the 72 ultimate-load results; the comparison therefore represents validation against a previously published experimental database rather than blind validation after database-specific calibration. The ratio of experimental to numerical ultimate load ranges from 0.83 to 1.08, with a mean of 0.952, a standard deviation of 0.045, RMSE of 68.2 kN, MAPE of 6.10%, and R2 = 0.937. A factorial evaluation of the validated matrix shows that additional CFRP layers increase peak load and deformation capacity, while concrete strength and steel tube thickness also exert strong effects. Stress contours indicate that CFRP confinement limits outward deformation and redistributes stresses, although these mechanistic conclusions remain conditional on the idealized perfect-bond interfaces and elastic CFRP representation. The framework is therefore suitable for trend-oriented studies within the investigated range, but it should not be extrapolated to cases involving different geometries, loading conditions, or explicit CFRP/interface failure without further validation.