This study prepared alkali-activated cementitious composites using high-whiteness kaolin, sodium water glass, and NaOH as the main raw materials. Multiple methods, including FE-SEM, XRD, whiteness/light transmittance tests, shrinkage rate measurements, DSC-TG, flexural strength testing, and hydrolysis resistance testing, were used to investigate the effects of curing temperature and time on material properties. The optimal parameters were determined as kaolin calcined at 1100 °C, activator modulus 1.25, calcined kaolin-to-activator ratio 1:1, and 2.5% deionized water added for molding. The optimal sample achieved a flexural strength of 23.81 MPa, with the bonding strength to porcelain 60.17 times that of gypsum and 1.90 times that of kaolin-bonded materials. Curing below 100 °C slowed polymerization, while temperatures exceeding 100 °C accelerated it, with violent reaction at 120 °C. Curing beyond 10 h reduced flexural strength. A large number of cage-like, ‘zeolite-like’ structures formed, closely relating to material properties. This study provides references for ceramic restoration materials.
This study investigates whether Yuan Dynasty Jingdezhen Luanbai glaze can support cobalt-blue coloration under conditions relevant to early blue-and-white porcelain production. Comparative analyses of archaeological Luanbai and blue-and-white specimens show that the two glaze types have similar average thicknesses, approximately 0.20 mm, and comparable basic chemical compositions, especially in their SiO2 and Al2O3 contents. These results suggest that they belong to related high-temperature calcium–alkali glaze traditions rather than completely isolated technological systems. Simulated firing experiments using five cobalt pigments of different compositions further indicate that Luanbai glaze can support cobalt-blue coloration at 1300 °C in a reducing atmosphere. Compared with unglazed controls, Luanbai-glazed samples showed a more consistent blue appearance and clearer pigment–glaze interaction. XPS and SEM-EDS line-scan analyses revealed differences in the near-surface chemical environment and cross-sectional distribution of Co, Mn, and Fe between glazed and unglazed samples, supporting the role of glaze coverage in color development. Refiring experiments on authentic Yuan sherds further supported the feasibility of cobalt-blue coloration on historical Luanbai glaze surfaces. Overall, the results suggest that the opalescent appearance of Luanbai glaze is not an inherent barrier to underglaze cobalt decoration. This work provides experimental evidence for reassessing the technological relationship between Luanbai and early blue-and-white porcelain.