One of the most studied deleterious phases in stainless steels is the sigma phase, due to its high potential to decrease the toughness and corrosion resistance of these steels. Eight samples of as-received cold rolled UNS S32205 duplex stainless steel were submitted to isothermal heat treatments at 850 oC during 10, 15, 30, 60, 120, 180, 240, and 300 minutes in order to study the precipitation kinetics of the sigma and chi deleterious phases. Several complementary microstructural analysis techniques were used to determine the volume fraction of the intermetallic phases, including optical microscopy and scanning electron microscopy (SEM) coupled with energy dispersive spectroscopy (EDS). Evaluation was made of the kinetics of isothermal formation of sigma and chi phases in commercial duplex stainless steels (UNS S32205). The results indicated two different mechanisms for sigma phase precipitation: sigma phase formed from the chi phase for shorter isothermal heat treatment times, and sigma phase precipitated at the ferrite-austenite interface for longer isothermal heat treatment times, using a temperature of 850 oC. The phase transformation kinetics determined using the JMA equation indicated that chi phase precipitation caused faster sigma phase formation.
29 November 2018 in Metallography, Microstructure, and Analysis
Duplex stainless steels are largely applied in petrochemical industries due to their high corrosion resistance and mechanical performance. Their applicability also requires a great wear resistance, which can be enhanced by friction stir processing (FSP), a surface hardening technique. In this work, FSP is utilized to process surfaces of UNS S32101 and UNS S32750. The materials were analyzed by EBSD in order to determine grain size and phase fraction. Microhardness tests were used to verify and compare the shifting of hardness values from 296 ± 8 to 314 ± 11 HV 0.2/15 and from 323 ± 8 to 350 ± 8 HV 0.2/15 for UNS S32101 and S32750, respectively. Abrasion tests were executed to study the wear behavior of both processed and unprocessed alloys. Abrasion tests indicated that the hardening by FSP promoted decrement of abrasive wear resistance. Volumetric loss increased after FSP, from 52.1 ± 0.5 to 53 ± 2 mm 3 , for UNS S32101, and from 50 ± 2 to 56.3 ± 0.3 mm 3 for UNS S32750. Tensile tests results were fitted to Hollomon's equation in order to identify mechanical properties and tendencies of strain hardening. SEM images were used to classify the wear micromechanisms acting on the samples. The results suggest that FSP can promote modifications of wear mechanisms and these changes can be correlated to the alloys' microstructure.