Basic wood density (BWD) is a functional characteristic important to quantify carbon storage and is related to tree growth and its survival. We investigated BWD variability among tree species, populations, and forest types across the Atlantic Forest biome in Rio de Janeiro state, Brazil. We sampled and measured 576 trees of 83 species in 28 natural ecosystems in the Dense Ombrophilous Forest, Seasonal Semi-deciduous Forest, and the Restinga Forest. Stem wood from two different heights at each tree was acquired using a drill borer; discs were removed from branches in 20% of the height from 39 trees. BWD means increased from 0.42 for the most humid ecosystem to 0.675 g⋅cm−3 from the driest ecosystem. We identified changes in the wood as a result of climatic variables particular to different typologies, such as increased wood density in areas with lower precipitation and higher temperatures, were also observed within species, but with little difference in means. We identified three groups of species according to their BWD, different in mean height and diameter. The branches can be used to estimate tree wood density.
This study aimed to evaluate the adhesion behavior of wood from an E. urophylla × E. grandis clone using the application of melamine–urea–formaldehyde (MUF), resorcinol–formaldehyde (RF), and polyurethane (PUR) adhesives in test samples obtained from 12 glulam beams. Adhesives were characterized by their pH, viscosity, density, and solid content. The wood–adhesive interface was assessed through the shear strength, percentage of wood failure, delamination, and photomicrograph analysis. A microdensitometer with X-rays and a resistograph were used to determine the material density and drilling resistance of the elements. Adhesive pH values ranged from 6.35 to 9.05. MUF exhibited the highest viscosity (1169 cP), while the adhesive density varied between 1.29 and 1.67 g cm−3. No statistically significant difference in results was obtained for the shear strength in dry conditions. The MUF adhesive showed a lower percentage of wood failure compared to PUR and RF. In the delamination test, the wood beams glued with RF yielded the best results. Photomicrographs revealed the adhesive’s penetration into the wood’s anatomical structure. Densitometry and resistograph profiles accurately represented the beam balancing configuration. The adhesives PUR, RF, and MUF demonstrated suitability for producing glulam beams with the Eucalyptus clone wood evaluated in this study.
The anatomical description of wood and charcoal for a wide variety of purposes is an essential tool for compiling databases to correctly identify species. This study describes and compares the anatomy of the wood and charcoal of Manilkara sp., collected in a protected area in the Pará state, Brazil. The qualitative anatomical characteristics of the wood, such as diffuse-porosity; vessels in radial multiples; alternate intervessel pits; axial parenchyma in lines or reticulate; rays uniseriate or biseriate, not storied, are corroborated in the literature. Moreover, this work reports the presence of helical thickenings in the vessel elements and possible helical thickenings in fibres in Manilkara. After the carbonization process, there were morphometric changes in the anatomical elements, as an increase in vessel frequency between 23 % and 141 %, and in ray frequency between 2.8 % and 12.9 %; while ray height decreased and ray width increased. Overall, some anatomical variations could be related to, or a result of the interaction between species plasticity, genetics, age and environmental factors. These characteristics enabled the identification of the samples at the genus level and the anatomical description of the wood and charcoal can be useful for forest inspections.