In this work, highly linear AlGaN/GaN laterally gated (or buried gate) high-electron-mobility transistors (HEMTs) are reported. The effect of gate dimensions on source-access resistance and the linearity of laterally gated devices are investigated experimentally in detail for the first time. Transistors with different gate dimensions and conventional planar devices are fabricated using two-step electron beam lithography (EBL). Current-voltage, source-access resistance, small-signal, and two-tone measurements are performed to evaluate the linearity of devices. Contrary to conventional planar HEMTs, the intrinsic transconductance of laterally gated devices monotonically increases with increasing gate voltage, showing a similar behavior as junction field-effect transistors (FETs). The source-access resistance shows a polynomial increase with the drain current, which can be reduced by decreasing the filling ratio of the buried gates. Through the optimization of these two competing factors, i.e., intrinsic transconductance and the source-access resistance, flat transconductance with high linearity is achieved experimentally. The laterally gated structure shows flat transconductance and small-signal power gain over a larger span of gate voltage that is 2.5 times higher than a planar device. Moreover, 6.9-dB improvement in output intercept point (OIP3)/P DC is achieved. This approach can be used to improve the linearity of AlGaN/GaN HEMTs at the device level.
24 July 2023 in IEEE Transactions on Electron Devices
N-polar GaN deep recess high electron mobility transistors (HEMTs) with metal-organic chemical vapor deposition (MOCVD) SiN $_\textit{x}$ SiN $\textit{x}$ gate dielectric have been shown to achieve record output powers and efficiencies in $\textit{W}$ -band. This study investigates the use of thermal atomic layer deposition (ALD) HfO $_{\text{2}}$ as the gate dielectric in deep recess N-polar GaN HEMTs for the first time. DC measurements showed a peak transconductance of 420 mS/mm, a gate leakage current of 140 nA/mm, and a dielectric breakdown field of 6.2 MV/cm. Importantly, near-zero hysteresis was observed in dc measurements and pulsed $\textit{I}$ – $\textit{V}$ measurements showed less than 5% dispersion. A unity current gain frequency ( $\textit{f}_{\textit{T}}\text{)}$ of 30.5 GHz and a maximum oscillation frequency ( $\textit{f}_{\text{MAX}}\text{)}$ of 53 GHz were measured. These results show the potential of using HfO $_{\text{2}}$ as a gate dielectric in the future ultra scaled N-polar deep recess GaN HEMTs.
1 March 2021 in Journal of Quantitative Spectroscopy and Radiative Transfer
In this article, heat generation distribution and maximum device temperature of gallium-nitride (GaN) high-electron-mobility transistors (HEMTs) are investigated by using the 2-D electrothermal and finite-element method (FEM) simulations. Devices with different gate lengths and source-to-drain spacing are investigated. It is observed that the maximum device temperature (TMAX) depends on the drain-to-source spacing and is almost independent of the gate length and that the assumption of a uniform heat generation region, under the gate, is not accurate; this is contrary to conventional calculation methods. Moreover, based on the results, a new approximation is proposed to use in the FEM simulations that can estimate TMAX more accurately. This method does not require physics-based technology computer-aided design (TCAD) simulations and can work with a low mesh density. The performance is compared with prior methods.
In this letter, we report a novel enhancement mode N-polar Deep Recess (NPDR) Gallium Nitride (GaN) High Electron Mobility Transistor (HEMT). Enhancement mode operation was achieved by recess etching with a combination of atomic layer etching (ALE) and wet etching. A high-k and high breakdown field HfSiO gate dielectric was employed. The epi-structure was grown on a low dislocation density on-axis N-polar GaN substrate by plasma-assisted molecular beam epitaxy (PAMBE). As a result, true normally-off operation with +0.8V threshold voltage, 1.5 A/mm peak saturation drain current, and 0.55 S/mm transconductance was achieved with 75 nm gate length (LG). A cutoff frequency (fT) of 122 GHz was measured, which resulted in a record fT*LG of 9.1 GHz $\cdot \mu $ m for E-mode AlGaN/GaN HEMTs. Load pull measurements demonstrated an output power of 2.7 W/mm and a power-added efficiency of 46% at 10 GHz.
In AlGaN/GaN high electron mobility transistors (HEMTs), high temperature processes (such as ohmic annealing with >800°C value) could deform the crystal structure and induce trap states within the bulk and surface. Expanded defect densities cause crucial problems, such as threshold voltage ( $\text{V}_{\text {th}}$ ) instability, current collapse, and high leakages. In this work, a low temperature ohmic contact process (630°C, 10 minutes) is adopted with recess etch, and contact resistances $< 0.1\Omega ~\cdot $ mm with low sheet resistances are achieved. The positive impact of this low thermal budget process on surface morphology, DC operation, long-term stability, and forward gate bias stress of the device is studied.