Conducting polymers are potential candidates for thermoelectric (TE) applications owing to their low thermal conductivity, non-toxicity and low cost. However, the coil conformation and random aggregation of polymer chains usually degrade electrical transport properties, thus deteriorating TE performance. In this work, we fabricated poly(3-hexylthiophene) (P3HT) films with highly oriented morphology using 1,3,5-trichlorobenzene (TCB), an organic small-molecule, as a template for polymer epitaxy under a temperature gradient crystallization process. The resulting P3HT molecules, which were confirmed to be highly anisotropic by a combination of scanning electron microscopy, atomic force microscopy, polarizing microscope, polarized Raman spectroscopy, and two-dimensional-grazing incidence X-ray diffraction (GIXRD) analysis, not only markedly reduced the conjugated defects along the polymer backbone, but also effectively increased the degree of electron delocalization. These combined phenomena produced an efficient, 1D path for carrier movement and therefore resulted in enhanced carrier mobility in the TCB-treated P3HT films. The maximum values of the electrical conductivity and Seebeck coefficient were 320 S cm−1 and 269 μV K−1, respectively. Consequently, the maximum TE power factor and ZT value at 365 K reached 62.4 μW mK−2 and 0.1, respectively, in the parallel direction of the TCB-treated P3HT film. To the best of our knowledge, these are the highest values reported for pure P3HT TE materials. The method of using organic small-molecule epitaxy to generate highly anisotropic polymer films is expected to be valid for many conducting polymers.
The development of flexible organic–inorganic thermoelectric composites constitutes a promising material approach toward harvesting heat from the human body or environment to power wearable electronics. To this end, compositing one-dimensional inorganic materials, such as carbon nanotubes or metal nanowires, with organic polymers has demonstrated efficacy but also drawbacks: e.g., the Seebeck coefficient of an inorganic constituent is too low to meet the onset voltage requirement of electronics, and it is hard to attain coherent interfaces between the inorganic and organic constituents. Here, we proposed a dimensionality/morphology matching strategy and conducted a proof-of-principle study on (PVDF)/Ta4SiTe4 organic–inorganic composites. A record high normalized maximum power density of 0.13 W m−1 at a temperature difference of 35.5 K was obtained in prototype flexible thermoelectric modules made of (PVDF)/Ta4SiTe4 composites. This study attests to the efficacy of the dimensionality/morphology matching strategy and the potential of using such conformal semiconducting organic–inorganic composites in wearable electronics.
In the past decade, the development of high-performance p-type flexible organic–inorganic thermoelectric composites based on nanocarbons (e.g., carbon nanotubes and graphene) has achieved unprecedented success, but progress in the n-type counterpart lags far behind because carbon nanotubes and graphene usually demonstrate p-type behavior. In this work, beyond carbon nanotubes and graphene, we conduct a proof-of-principle study using semiconducting graphdiyne (GDY) to fabricate high-performance n-type organic–inorganic flexible thermoelectric composites. Based on the chemical interactions between GDY and the quasi-one-dimensional semiconductor Ta4SiTe4, we successfully fabricate n-type Ta4SiTe4/polyvinylidene fluoride (PVDF)/GDY composite films. GDY is homogeneously distributed inside the composites, acting as bridges among the Ta4SiTe4 whiskers to significantly improve the electrical conductivity. Combining the well-maintained large Seebeck coefficient and low thermal conductivity, the Ta4SiTe4/PVDF/GDY composite films demonstrate a maximum ZT value of 0.2 at 300 K, among the highest reported in organic–inorganic flexible thermoelectric composites. The protype thermoelectric module that consists of n-type Ta4SiTe4/PVDF/GDY legs and p-type PEDOT:PSS/CNT legs shows the highest normalized maximum power density among the reported organic material-based flexible thermoelectric modules including both n- and p-type legs.
30 May 2018 in Angewandte Chemie International Edition
The fundamental understanding of the influence of molecular structure on the carrier transport properties in the field of organic thermoelectrics (OTEs) is a big challenge since the carrier transport behavior in conducting polymers reveals average properties contributed from all carrier transport channels, including those through intra-chain, inter-chain, inter-grain, and hopping between disordered localized sites. Here, combining molecular dynamics simulations and experiments, we investigated the carrier transport properties of doped highly oriented poly(3-hexylthiophene) (P3HT) films with different side-chain regioregularity. It is demonstrated that the substitution of side chains can not only take effect on the carrier transport edge, but also on the dimensionality of the transport paths and as a result, on the carrier mobility. Conductive atomic force microscopy (C-AFM) study as well as temperature-dependent measurements of the electrical conductivity clearly showed ordered local current paths in the regular side chain P3HT films, while random paths prevailed in the irregular sample. Regular side chain substitution can be activated more easily and favors one-dimensional transport along the backbone chain direction, while the irregular sample presents the three-dimensional electron hopping behavior. As a consequence, the regular side chain P3HT samples demonstrated high carrier mobility of 2.9 ± 0.3 cm2/V·s, which is more than one order of magnitude higher than that in irregular side chain P3HT films, resulting in a maximum thermoelectric (TE) power factor of 39.1 ± 2.5 μW/mK2 at room temperature. These findings would formulate design rules for organic semiconductors based on these complex systems, and especially assist in the design of high performance OTE polymers.