Low-temperature properties of high-density polyethylene (HDPE), low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), and their blends were studied. The analyzed low-temperature mechanical properties involve the deformation resistance and impact strength characteristics. HDPE is a bimodal ethylene/1-hexene copolymer; LDPE is a branched ethylene homopolymer containing short-chain branches of different length; LLDPE is a binary ethylene/1-butene copolymer and an ethylene/1-butene/1-hexene terpolymer. The samples of copolymers and their blends were studied by gel permeation chromatography (GPC), differential scanning calorimetry (DSC), 13C NMR spectroscopy, and dynamic mechanical analysis (DMA) using testing machines equipped with a cryochamber. It is proposed that such parameters as “relative elongation at break at −45 °C” and “Izod impact strength at −40 °C” are used instead of the ductile-to-brittle transition temperature to assess frost resistance properties because these parameters are more sensitive to deformation and impact at subzero temperatures for HDPE. LLDPE is shown to exhibit higher relative elongation at break at −45 °C and Izod impact strength at −20 ÷ 60 °C compared to those of LDPE. LLDPE terpolymer added to HDPE (at a content ≥ 25 wt.%) simultaneously increases flow properties and improves tensile properties of the blend at −45 °C. Changes in low-temperature properties as a function of molecular weight, MWD, crystallinity, and branch content were determined for HDPE, LLDPE, and their blends. The DMA data prove the resulting dependences. The reported findings allow one to understand and predict mechanical properties in the HDPE–LLDPE systems at subzero temperatures.
Comparative studies of the structure and thermal behavior of cellulose and composite precursors with additives of silyl-substituted acetylene and alkoxysilanes were carried out. It is shown that the introduction of silicon-containing additives into the cellulose matrix influenced the thermal behavior of the composite fibers and the carbon yield after carbonization. Comparison of the activation energies of the thermal decomposition reaction renders it possible to determine the type of additive and its concentration, which reduces the energy necessary for pyrolysis. It is shown that the C/O ratio in the additive and the presence of the Si–C bond affected the activation energy and the temperature of the beginning and the end of the pyrolysis reaction.
Replacing the aqueous coagulation bath with an alcoholic one during spinning cellulose fibers (films) from solutions in N-methylmorpholine-N-oxide leads to a radical restructuring of the hydrogen bonds net of cellulose and, as a result, to a change in the structure and properties of the resulting material. By the method of optical interferometry, it was possible to identify the intrinsic features of the interaction of the solvent and isomeric alcohols and to construct phase diagrams of binary systems describing the crystalline equilibrium. Knowledge of the phase states of the system at different temperatures renders it possible to exclude the process of solvent crystallization and conduct the spinning in pseudo-homogeneous conditions. The structure and morphology of samples were studied using X-ray diffraction and scanning electron microscopy methods for a specific coagulant. When the solution under certain conditions is coagulated at contact with alcohol, the solvent may be in a glassy state, whereas, when at coagulation in water, an amorphous-crystalline structure is formed. The structural features of cellulose films obtained by coagulation of solutions with water and alcohols help to select potential engineering or functional materials (textile, packaging, membranes, etc.), in which their qualities will manifest to the best extent.
22 May 2006 in Macromolecular Chemistry and Physics