The application of laser powder bed fusion (LPBF) to 7xxx-series aluminum alloys is fundamentally limited by hot cracking and porosity. This study demonstrates that adding 5 wt.% AlCoCrFeNi2.1 high-entropy alloy (HEA) particles to 7075 aluminum alloy (AA7075) powder can effectively mitigate these issues. Microstructural characterization revealed that the HEA particles remained largely intact and formed a strong metallurgical bond with the α-Al matrix. Scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS) analysis confirmed that this bonding is facilitated via the in situ formation of new intermetallic phases at the particle/matrix interface. X-ray diffraction (XRD) identified these phases as primarily Al5Co2 and Fe3Ni2. A key consequence of this reinforced interface is a significant change in cracking behavior; optical microscopy (OM) showed that long, continuous cracks typical of AA7075 were replaced by shorter, deflected cracks in the composite. While porosity was not eliminated, the addition of HEA stabilized the process, yielding a consistent density improvement of 0.5–1.5% across the processing window. This microstructural modification resulted in a substantial ~64% increase in average microhardness, which increased from 96.41 ± 9.81 HV0.5 to 158.46 ± 11.33 HV0.5. These results indicate that HEA reinforcement is a promising route for engineering the microstructure and improving the LPBF processability of high-strength aluminum alloys.
Laser powder bed fusion (LPBF) of AA7075 is severely constrained by a narrow process window and susceptibility to defect formation (hot cracking and porosity), which often dominates performance. In this study, 5 wt.% AlCoCrFeNi2.1 high-entropy alloy (HEA) particles, volumetric energy density (VED = 74–222 J·mm−3), and subsequent T6 heat treatment were systematically investigated to reveal their combined effects on defect structure, crystallographic texture/substructure, and tensile behaviour. Quantitative EBSD shows a measurable grain refinement in the as-built state (average grain size 13.44 → 11.80 µm, ~12%) accompanied by a pronounced weakening of the fibre texture (maximum MRD 4.94 → 2.38), indicating disrupted epitaxial growth and a more dispersed orientation distribution. After T6, the reinforced alloy retains a higher low-angle boundary fraction (31.62% vs. 24.17% in unreinforced AA7075) and a higher kernel average misorientation (0.80° vs. 0.60°), consistent with particle-stabilised substructure retention and retarded recovery. Across all VEDs, AA7075-HEA exhibits higher microhardness (compared with AA7075, the addition of HEA increases the hardness by roughly 20–50 HV) and tensile strength, with the intermediate VED (140.74 J·mm−3, T6 states) yielding the best performance. While macroscopic cracking is not fully eliminated, the results clarify that HEA-enabled texture/substructure modifications can contribute to enhanced defect tolerance and are more effectively translated into tensile performance when the as-built defect severity is controlled. These findings provide quantitative insights into defect–microstructure–property coupling in LPBF AA7075-HEA composites from as-built to T6 states.