In this study, gamma irradiation induced degradation of orange peels (OP) was investigated. The lignocellulosic biomass degradation was carried out at doses of 0 (control), 600, 1800 and 3500 kGy using a Co-60 gamma radiation source. The samples were tested for total and reducing sugars. The concentrations of total sugars ranged from 0.530 g∙g−1 in control sample to 0.382 g∙g−1 of dry weight in the sample which received the highest radiation dose. The reducing sugars content varying from 0.018 to 0.184 g∙g−1 of dry weight with the largest rise occurring in the sample irradiated at 3500 kGy. The concentrations of sucrose, glucose and fructose were determined. The changes generated in physico-chemical properties were determined by Fourier Transform Infrared Spectroscopy (FTIR) and termogravimetric analysis (TG-DTG). The results show that OP was affected, but not significantly, which suggests that lignocellulose and sugars profiles were partially degraded after gamma irradiation.
24 June 2021 in Journal of Applied Polymer Science
Poly(methyl methacrylate) (PMMA) is one of the most commonly plastics used as dental-base material, due to its good biological compatibility and mechanical properties. Chitosan has wide application in chemical, biochemical and biomedical fields of research. In this work, chitosan (CTS) was functionalized with glycidyl methacrylate (GMA), to ease a further reaction with MMA. The resulting co-polymer was finally blended with PMMA and poly(butyl acrylate) PBA which works as a damper, the polymers were cured by UV to obtain the final resin. Characterization of UV-cured resins was carried out by thermal measurements, X-ray diffraction, atomic force microscopy (AFM), micro and nanoindentation, water absorption and elution in water. As a result a higher thermal stability of the final resin compared with the precursor co-polymer ((CTS-GMA)-g-PMMA) was obtained. The resin presented roughness in the nanometer scale and nanoparticles embedded in the acrylic matrix producing a tough material. However, XRD measurements show that all materials are in an amorphous state. Values of hardness and elastic modulus results were very near to those of the dentine. The results of elution in water of the tested resin samples show them as clinically acceptable as a dental base material.
9 July 2024 in Journal of the Science of Food and Agriculture