Direct metal laser sintering (DMLS) is a technique to manufacture complex functional mechanical parts from a computer-aided design (CAD) model. Usually, the mechanical components produced by this procedure show higher residual porosity and poorer mechanical properties than those obtained by conventional manufacturing techniques. In this work, a Co-Cr-Mo alloy produced by DMLS with a composition suitable for biomedical applications was submitted to hardness measurements and structural characterization. The alloy showed a hardness value remarkably higher than those commonly obtained for the same cast or wrought alloys. In order to clarify the origin of this unexpected result, the sample microstructure was investigated by X-ray diffraction (XRD), electron microscopy (SEM and TEM) and energy dispersive microanalysis (EDX). For the first time, a homogeneous microstructure comprised of an intricate network of thin ε (hcp)-lamellae distributed inside a γ (fcc) phase was observed. The ε-lamellae grown on the {111}γ planes limit the dislocation slip inside the γ (fcc) phase, causing the measured hardness increase. The results suggest possible innovative applications of the DMLS technique to the production of mechanical parts in the medical and dental fields.
1 July 2016 in Journal of the Mechanical Behavior of Biomedical Materials
Direct Metal Laser Sintering (DMLS) technology was used to produce tensile and flexural samples based on the Ti-6Al-4V biomedical composition. Tensile samples were produced in three different orientations in order to investigate the effect of building direction on the mechanical behavior. On the other hand, flexural samples were submitted to thermal treatments to simulate the firing cycle commonly used to veneer metallic devices with ceramics in dental applications. Roughness and hardness measurements as well as tensile and flexural mechanical tests were performed to study the mechanical response of the alloy while X-ray diffraction (XRD), electron microscopy (SEM, TEM, STEM) techniques and microanalysis (EDX) were used to investigate sample microstructure. Results evidenced a difference in the mechanical response of tensile samples built in orthogonal directions. In terms of microstructure, samples not submitted to the firing cycle show a single phase acicular α' (hcp) structure typical of metal parts subject to high cooling rates. After the firing cycle, samples show a reduction of hardness and strength due to the formation of laths of the β (bcc) phase at the boundaries of the primary formed α' plates as well as to lattice parameters variation of the hcp phase. Element partitioning during the firing cycle gives rise to high concentration of V atoms (up to 20wt%) at the plate boundaries where the β phase preferentially forms.
Laser-based powder bed fusion (L-PBF) is an additive manufacturing (AM) technique that uses a computer-controlled laser beam as the energy source to consolidate a metal powder according to a layer-upon-layer strategy in order to manufacture a three dimensional part. This opens the way for an unprecedented freedom in geometry, but the layer-wise build-up strategy typically results in a very poor surface finish, which is affected by the staircase effect and by the presence of partially molten particles. Surface finishing treatments are therefore necessary to obtain an adequate surface finish, to improve the fatigue behavior and to meet mechanical and aesthetic needs. The present contribution systematically compares numerous surface finishing techniques, including laser shock processing, plastic media blasting, sand blasting, ceramic shot peening and metal shot peening with steel particles of different sizes (ϕ = 0.2 mm and ϕ = 0.4 mm). The results show that all the proposed methods improve the surface quality and the fatigue life of A357.0 L-PBF parts. However, the achievement of the lowest surface roughness does not necessarily correspond to the best fatigue performance, thus suggesting that multiple mechanisms may be active and that besides surface roughness also residual stresses contribute to increase the fatigue strength.