This article investigated the influence of the incorporation of metakaolin in paving blocks. Two methods of incorporation were conducted in two factories. The first method consisted of addition with 10, 15, 20, 25, and 30% metakaolin in relation to the amount of cement, and the second one analysed the partial replacement of cement in the contents of 4, 8, and 10%. The results showed that in mixtures with replacement, the metakaolin did not show improvements in all properties. In contrast, in cases with addition, the compressive strength improved, and absorption was reduced. In both methods, the abrasion resistance did not change with the incorporation of metakaolin. Finally, the addition of 10% proved to be sufficient for application in paving blocks.
22 October 2023 in Journal of Building Engineering
This comprehensive study meticulously evaluated six probability distribution models for the compressive strength of 24 concrete blocks, 12 with metakaolin and 12 without addition. The models analyzed were Lognormal, Gamma, Normal, Weibull, Beta, and Exponential. For blocks with metakaolin, the Lognormal distribution presented the best fit, followed by Gamma, Normal, Beta, and Weibull, while the Exponential needed to be more adequate. In blocks without metakaolin, the Gamma distribution was the most efficient, followed by Normal, Weibull, Lognormal, and Beta, with the Exponential also inadequate. The model parameters were adjusted based on the resistance frequencies estimated for each group of samples. Thus, Lognormal and Gamma performed better in predicting compressive strength, depending on the presence or absence of metakaolin. The Exponential distribution, in turn, was considered inadequate in both cases.
The present work investigated the effect of different storage temperatures (10 °C, 30 °C, and 50 °C) on the mechanical, structural, chemical, and microstructural properties of a set of sustainable mortars with gray waste. Three types of mortar were investigated: (1) Type A, prepared from a proportion of 1 part cement: 1 part hydrated lime: 6 parts sand; (2) Type B, prepared from a proportion of 1 part cement: 1 part hydrated lime: 6 parts sand: 0.1 part waste; and (3) Type C, prepared from a proportion of 0.9 part cement: 1 part hydrated lime: 6 parts sand: 0.1 part waste. The waste incorporation reduced compressive strength by 8%, while partial cement replacement reduced by 33%. The cement storage at 10 °C preserved the compressive strength, whereas storage at 50 °C increased it by 8.8%. In type B mortar, the waste incorporation improved compressive strength by 19% at 50 °C. The most substantial enhancement occurred in type C mortar, where cement replacement with residue and storage at 50 °C led to a 27% increase. These results highlight the potential of higher storage temperatures to mitigate cement degradation in humid environments. Furthermore, XRD analysis revealed that cement storage temperature did not affect the formation of primary cement phases, as degradation products were chemically similar to hydration products. However, sustainable mortars exhibited changes in the C-S-H phase signal when the cement is stored for 90 days at 30 °C. Finally, SEM and EDS analyses identified variations in Ca, Si, and O proportions depending on storage conditions.
1 August 2024 in Contribuciones A Las Ciencias Sociales
This study investigates waste glass (WG) as an environmentally friendly substitute for natural sand in cement mixtures. Plastering mortars were fabricated by replacing sand with WG at proportions of 10%, 20%, and 30%. X-ray diffraction, Thermogravimetry, Scanning Electron Microscopy, and Energy-dispersive X-ray spectroscopy characterized the mortars. Compressive strength was measured at two ages (7 and 28 days) for WG-containing mortars. Results confirm the suitability of waste glass as a sand replacement in mortars, with the 20% WG sample showing optimal compressive strength, contributing to environmental and economic impact reduction. Thermogravimetric analysis of the 30% WG mortar shows a significant difference in mass loss percentages compared to the reference mortar, losing only 3.65% at 28 days versus 7.85%. Additionally, waste glass increased mortar density, reducing porosity and enhancing structural uniformity. Despite a decrease in compressive strength values, the results remain satisfactory for application in the Civil Construction industry. This comprehensive exploration underscores the potential of waste glass as a sustainable alternative, emphasizing its positive effects on both performance and environmental considerations.