The recent increase in end-of-life (EoL) lithium-ion batteries (LiBs) has become a significant concern worldwide. Most studies in the literature have primarily focused on recovering cathode active metals from black mass (BM), whereas the separation of anode–cathode foils, plastics, and casing metals which are the essential components of LiBs has received relatively little attention. To reduce costs and maximize the recovery of valuable metals in subsequent hydrometallurgical or pyrometallurgical processes, EoL LiBs require appropriate pre-treatment. This study aims to scrape off the BM adhering to the electrode foils resulting from gradual crushing and subsequently separate the plastics and copper (Cu) from other metals through a two-step selective flotation process. The results demonstrated that plastics, due to their natural hydrophobicity, could be effectively removed using a frother, achieving more than 95% recovery with less than 5% metallic contamination. Following plastic flotation, Cu particles were floated in the presence of 3418A, yielding a Cu concentrate containing 65.13% Cu with a recovery rate of 96.4%. Additionally, the aluminum (Al) content in the non-floating material, remaining in the cell, increased to approximately 77%.
The recent increase in end-of-life (EoL) lithium-ion batteries (LiBs) has become a significant concern worldwide. Most studies in the literature have primarily focused on recovering cathode active metals from black mass, whereas the separation of anode–cathode foils, plastics, and casing metals which are the essential components of LiBs has received relatively little attention. To reduce costs and maximize the recovery of valuable metals in subsequent hydrometallurgical or pyrometallurgical processes, EoL LiBs require appropriate pre-treatment. This study aims to scrape off the black mass (battery dust) adhering to the electrode foils resulting from gradual crushing and subsequently separate the plastics and copper (Cu) from other metals through a two-step selective flotation process. The results demonstrated that plastics, due to their natural hydrophobicity, could be effectively removed using a frother. Following plastic flotation, Cu particles were floated in the presence of Aerophine 3418A, yielding a Cu concentrate containing 65.13% Cu with a recovery rate of 96.4%. Additionally, the aluminum (Al) content in the non-floating material, remaining in the cell, increased to approximately 77%.
The increase in end-of-life (EoL) Lithium-ion Batteries (LIBs) in recent times has become a major concern for the global community. Most of the research in the literature has focused on the recovery of cathode active metals from black mass. The separation of anode-cathode foils, plastics, and casing metals, which are essential parts of LIBs, remained limited. To reduce costs and maximize the recovery of valuable metals in the subsequent hydro or pyro metallurgical processes EoL LIBs need to be pre-treated accordingly. The main purpose of this study is to scrape off the black mass (or battery dust) adhering to the electrode foils as a result of gradual crushing and then to separate the plastic and copper from other metals by two-step selective flotation. The results showed that plastics with natural hydrophobicity could be removed with the help of a frother. After plastic flotation, the copper particles were floated in the presence of Aerophine 3418A, and a copper concentrate assaying 65.13% Cu was obtained with 96.4% Cu recovery at the end of the copper flotation circuit. In addition, the Al content in the material that could not float and remained in the cell was increased to approximately 77%.