The refractory tungsten alloys with high ductility/strength/plasticity are highly desirable for a wide range of critical applications. Here we report an interface design strategy that achieves 8.5 mm thick W-0.5 wt. %ZrC alloy plates with a flexural strength of 2.5 GPa and a strain of 3% at room temperature (RT) and ductile-to-brittle transition temperature of about 100 °C. The tensile strength is about 991 MPa at RT and 582 MPa at 500 °C, as well as total elongation is about 1.1% at RT and as large as 41% at 500 °C, respectively. In addition, the W-ZrC alloy plate can sustain 3.3 MJ/m2 thermal load without any cracks. This processing route offers the special coherent interfaces of grain/phase boundaries (GB/PBs) and the diminishing O impurity at GBs, which significantly strengthens GB/PBs and thereby enhances the ductility/strength/plasticity of W alloy. The design thought can be used in the future to prepare new alloys with higher ductility/strength.
Nowadays it is commonly considered that high damping materials which have both the good mechanical properties as structural materials and the high damping capacity for vibration damping are the most direct vibration damping solution. In metals and alloys however, exhibiting simultaneously high damping capacity and good mechanical properties has been noted to be normally incompatible because the microscopic mechanisms responsible for internal friction (namely damping capacity) are dependent upon the parameters that control mechanical strength. To achieve a compromise, one of the most important methods is to develop two-phase composites, in which each phase plays a specific role: damping or mechanical strength. In this review, we have summarized the development of the design concept of high damping composite materials and the investigation of their fabrication and properties, including mechanical and damping properties, and suggested a new design concept of high damping composite materials where the hard ceramic additives exhibit high damping capacity at room temperature owing to the stress-induced reorientation of high density point defects in the ceramic phases and the high damping capacity of the composite comes mainly from the ceramic phases.
21 June 2010 in The Journal of Physical Chemistry C
Structure and magnetic properties of undoped PrMnO3+δ nanoparticles with average particle size ranging from 40–500 nm have been investigated. Compared with bulk PrMnO3 compound with A type antiferromagnetic ordering below TN=95 K, PrMnO3+δ nanoparticles exhibit ferromagnetic ordering. With decreasing particle size, the MnO6 octahedra distortion increases, the cell volume shrinks, the average Mn–O bond length increases and the Mn–O–Mn bond angle decreases; the ferromagnetism becomes weak and the Curie temperature decreases gradually, and meanwhile, the spin glass behavior becomes more obvious. However, in contrast to antiferromagnetic nanoparticles, no exchange bias phenomenon was observed in our case. These interesting results are attributed to the excessive oxygen content and surface effects.