Phenol, an essential feedstock widely used in manufacturing and chemical industries, inevitably results in the discharge of phenol-laden wastewater. To enhance the phenol-degradation efficiency of Fe-based amorphous alloys, a novel atomic-scale fabrication approach for Fe-Cu galvanic couples is proposed, enabling the rapid and uniform formation of micro/nano Fe-Cu structures on the surface of Fe-based alloys with significant improvement in the catalytic activity towards phenol. Micron/nano Fe-Cu couples can be fabricated within 15 s at 45 °C. Phenol degradation experiments reveal that the pristine amorphous alloy exhibits a 40 min hatching period before the phenol removal process, and it exhibits a kinetic constant (kobs) of 0.1596 min−1 after the hatching period, under conditions of 50 °C, 0.5 g/L catalytic loading, 10 mmol/L H2O2, and pH = 3 towards a 50 mg/L phenol solution. With the micro/nano Fe-Cu galvanic couples, the kobs value markedly increased to 2.23~2.36 min−1 under identical conditions except for 3 mmol/L H2O2, corresponding to approximately a 14-fold improvement. This cost-effective and time-efficient atomic-scale fabrication strategy offers a promising platform for the development of next-generation catalytic alloys and functional materials.
Molybdenum (Mo) finds extensive applications in the steel industry, and the recycling of secondary molybdenum resources is crucial for the green development of the molybdenum sector. Meanwhile, the large-scale stockpiling of copper slag, a bulk industrial solid waste, poses severe environmental and resource-related challenges. Addressing the common issues of the refractory nature of waste molybdenum disilicide (MoSi2) and the underutilization of iron resources in copper slag, this study proposes a synergistic smelting approach using copper slag and waste MoSi2, aiming to realize the coordinated treatment of these two solid wastes and the simultaneous, efficient recovery of valuable metals (Mo and Fe). Under non-isothermal conditions, this work elucidates the phase evolution of copper slag and the decomposition–reduction behavior of MoSi2; clarifies the dual role of coke as the primary reductant at the initial reaction stage and as a maintainer of a reducing atmosphere during smelting; and systematically investigates the effects of smelting temperature, slag basicity, and coke dosage on metal recovery. The results demonstrate that, under optimized process conditions, the recovery efficiencies of molybdenum and iron can reach 98.97% and 98.46%, respectively. This study provides a new strategy for the enrichment and extraction of metallic elements from waste MoSi2 and copper slag.