Tribological properties of TiN and CrN coatings deposited by cathodic arc method at three different bias potentials -50, -150 and -300V on Ti-6Al-4V alloy in pair with alumina have been investigated. X-ray diffraction analysis showed that single-phase textured cubic nitrides of TiN and CrN were formed in these coatings. It is shown that the friction coefficient of the coatings is practically equal to that established for the Ti6Al4V alloy, but the wear rate is more than an order of magnitude lower than for the titanium alloy substrate. Coatings deposited at a potential of -50 V show optimal tribological properties at temperatures 20 and 500°C. Friction coefficients for TiN coatings are 0.4-0.8 at 20°C and 0,75 at 500°C; for CrN coatings they are 0.5 at 20°C and 0,7 at 500°C. Wear rates for TiN coatings are 0.86·10-5 мм3/Нм at 20°C and 3.56·10-5 мм3/Нм at 500°C; for CrN coatings they are 1.43·10-5 мм3/Нм at 20°C and 7.13·10-5 мм3/Нм at 500°C.
The V-O-N coating set was produced at different relative oxygen concentrations of O2(x) = O2/(N2 +O2) using cathodic arc evaporation. The aim of the research was to determine the effect of oxygen on coating properties. The coatings’ composition and structural properties (X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX)) and mechanical properties—hardness, adhesion, and wear resistance (nano-indenter, scratch tester, ball-on-disc tester)—were extensively investigated. EDX and XRD analyses indicate that in coatings formed with a relative oxygen concentration in the range of 20–30%, the oxygen concentration in the coating increases dramatically from approximately 16 at.%. to 63 at.%, and the nitrogen concentration drops from about 34 at.% up to 3 at.%. This may indicate greater activity of oxygen compared to nitrogen in forming compounds with vanadium. The occurrence of the V5O9 phase belonging to the Magnéli phases was observed. Microscopic observations indicate that the number of surface defects increases with the oxygen concentration in the coating. The opposite effect is characterized by mechanical properties—hardness, adhesion, and wear resistance decrease with increasing oxygen concentration in the coating.
9 March 2026 in Physicochemical Mechanics of Materials
The composition, structure, mechanical characteristics, long-term oxidation resistance and electrical conductivity of coatings produced by vacuum-arc deposition method using a cathode (target) made of Ti–6.1Al–5.5Zr–2.3Sn–0.8Mn–0.6Si–0.4Mo–0.3Nb titanium alloy were studied. The coatings were deposited on a 0.5 mm thick substrate made of a cost-effective Ti–2.2Al–1.5Mn–0.3Zr–0.3Fe–0.1C alloy at a substrate bias voltage Ubias = –50…–200 V. The properties of the materials were compared in the as-received state and after long-term holding for 1000 h at 600°C in air, simulating the effect of the cathode environment in solid oxide fuel cells (SOFCs). It was established that the plates with a 10 mm thick coating at Ubias = -100 V exhibit high oxidation resistance (Δm/S = 0.88 mg/cm2) and surface electrical conductivity in the oxidized state (σ = 2.4×105 S/m) and meet the requirements for lightweight interconnect materials in cathode side of intermediate-temperature SOFCs.
Tribological properties of TiN and CrN coatings deposited by cathodic arc method at three different bias potentials -50, -150 and -300V on Ti-6Al-4V alloy in pair with alumina have been investigated. The wear rate of the coatings is more than an order of magnitude lower than for the titanium alloy substrate. The friction coefficient is in the range of 0.4-0.8 for TiN coatings and 0.5 for CrN coatings. Coatings deposited at a potential of -50 V show optimal tribological properties.